Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
CONSTRUCTION METHOD FOR WATER RETENTIVE PAVEMENT
To provide a construction method for cast-in-place water retentive pavement which can be installed in a short time with less labor.SOLUTION: A construction method for a cast-in-place water retentive pavement, comprises the steps of: coating concrete or a steel floor slab with an organic adhesive; spreading water-retentive cement milk on a coated surface; placing porous concrete so that a (lower) part of the porous concrete is immersed in the water-retentive cement milk; and spreading and compacting the porous concrete, followed by curing. In the porous concrete, the unit quantity of cement is 125 to 950 kg/m, the unit quantity of fine aggregate is 40 to 350 kg/m, the unit quantity of coarse aggregate is 1100 to 2100 kg/m, the unit quantity of water is 20 to 180 kg/m, the unit quantity of thickener or underwater-inseparable admixture is 0.5 to 6.0 kg/m, and the compounded amount of high-performance water reducing agent or high-performance AE water reducing agent with respect to cement is 1.7 to 6.0 mass%.SELECTED DRAWING: Figure 1
【課題】短時間で少ない労力で施工ができる現場打ち保水性舗装の施工方法を提供する。【解決手段】コンクリート又は鋼床版上に有機系接着剤を塗布する工程、塗布面に保水性セメントミルクを敷き均す工程、ポーラスコンクリートの一部(下部)が、前記保水性セメントミルクに浸されるようにポーラスコンクリートを打設する工程、ポーラスコンクリートを締固めて敷き均した後、養生する工程を含む現場打ち保水性舗装の施工方法であって、ポーラスコンクリートが、セメントの単位量が125〜950kg/m3、細骨材の単位量が40〜350kg/m3、粗骨材の単位量が1100〜2100kg/m3、水の単位量が20〜180kg/m3、増粘剤又は水中不分離性混和剤の単位量が0.5〜6.0kg/m3、および高性能減水剤又は高性能AE減水剤の配合量がセメントに対して1.7〜6.0質量%である。【選択図】図1
CONSTRUCTION METHOD FOR WATER RETENTIVE PAVEMENT
To provide a construction method for cast-in-place water retentive pavement which can be installed in a short time with less labor.SOLUTION: A construction method for a cast-in-place water retentive pavement, comprises the steps of: coating concrete or a steel floor slab with an organic adhesive; spreading water-retentive cement milk on a coated surface; placing porous concrete so that a (lower) part of the porous concrete is immersed in the water-retentive cement milk; and spreading and compacting the porous concrete, followed by curing. In the porous concrete, the unit quantity of cement is 125 to 950 kg/m, the unit quantity of fine aggregate is 40 to 350 kg/m, the unit quantity of coarse aggregate is 1100 to 2100 kg/m, the unit quantity of water is 20 to 180 kg/m, the unit quantity of thickener or underwater-inseparable admixture is 0.5 to 6.0 kg/m, and the compounded amount of high-performance water reducing agent or high-performance AE water reducing agent with respect to cement is 1.7 to 6.0 mass%.SELECTED DRAWING: Figure 1
【課題】短時間で少ない労力で施工ができる現場打ち保水性舗装の施工方法を提供する。【解決手段】コンクリート又は鋼床版上に有機系接着剤を塗布する工程、塗布面に保水性セメントミルクを敷き均す工程、ポーラスコンクリートの一部(下部)が、前記保水性セメントミルクに浸されるようにポーラスコンクリートを打設する工程、ポーラスコンクリートを締固めて敷き均した後、養生する工程を含む現場打ち保水性舗装の施工方法であって、ポーラスコンクリートが、セメントの単位量が125〜950kg/m3、細骨材の単位量が40〜350kg/m3、粗骨材の単位量が1100〜2100kg/m3、水の単位量が20〜180kg/m3、増粘剤又は水中不分離性混和剤の単位量が0.5〜6.0kg/m3、および高性能減水剤又は高性能AE減水剤の配合量がセメントに対して1.7〜6.0質量%である。【選択図】図1
CONSTRUCTION METHOD FOR WATER RETENTIVE PAVEMENT
保水性舗装の施工方法
KISHIRA RYO (Autor:in) / KAJIO SATOSHI (Autor:in) / HIGUCHI TAKAYASU (Autor:in)
06.06.2019
Patent
Elektronische Ressource
Japanisch
IPC:
E01C
Bau von Straßen, Sportplätzen oder dgl., Decken dafür
,
CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, OR THE LIKE
INJECTION MATERIAL FOR WATER RETENTIVE PAVEMENT AND WATER RETENTIVE PAVEMENT BODY
Europäisches Patentamt | 2017
|