PRODUCTION METHOD OF SEMI-CURED COMPOSITE, METHOD FOR PRODUCING CURED COMPOSITE, AND SEMI-CURED COMPOSITE
To suppress a rapid rise in the viscosity of a semi-cured material in a semi-cured composite in which a porous material is impregnated with a semi-cured material of a curable composition.SOLUTION: An aspect of the present invention provides a method for producing a semi-cured composite, comprising the steps of: impregnating a porous body with a curable composition containing a first polymerizable component, a first polymerization initiator for initiating the polymerization of the first polymerizable component, a second polymerizable component, and a second polymerization initiator for initiating the polymerization of the second polymerizable component under conditions different from those of the first polymerization initiator; and polymerizing the first polymerizable component with the first polymerization initiator.SELECTED DRAWING: None
【課題】多孔質体に硬化性組成物の半硬化物が含浸された半硬化物複合体において、半硬化物の粘度の急激な上昇を抑制すること。【解決手段】本発明の一側面は、第1の重合性成分と、第1の重合性成分の重合を開始させる第1の重合開始剤と、第2の重合性成分と、第1の重合開始剤とは異なる条件で第2の重合性成分の重合を開始させる第2の重合開始剤と、を含有する硬化性組成物を多孔質体に含浸させる工程と、第1の重合性成分を、第1の重合開始剤により重合させる工程と、を備える、半硬化物複合体の製造方法を提供する。【選択図】なし
PRODUCTION METHOD OF SEMI-CURED COMPOSITE, METHOD FOR PRODUCING CURED COMPOSITE, AND SEMI-CURED COMPOSITE
To suppress a rapid rise in the viscosity of a semi-cured material in a semi-cured composite in which a porous material is impregnated with a semi-cured material of a curable composition.SOLUTION: An aspect of the present invention provides a method for producing a semi-cured composite, comprising the steps of: impregnating a porous body with a curable composition containing a first polymerizable component, a first polymerization initiator for initiating the polymerization of the first polymerizable component, a second polymerizable component, and a second polymerization initiator for initiating the polymerization of the second polymerizable component under conditions different from those of the first polymerization initiator; and polymerizing the first polymerizable component with the first polymerization initiator.SELECTED DRAWING: None
【課題】多孔質体に硬化性組成物の半硬化物が含浸された半硬化物複合体において、半硬化物の粘度の急激な上昇を抑制すること。【解決手段】本発明の一側面は、第1の重合性成分と、第1の重合性成分の重合を開始させる第1の重合開始剤と、第2の重合性成分と、第1の重合開始剤とは異なる条件で第2の重合性成分の重合を開始させる第2の重合開始剤と、を含有する硬化性組成物を多孔質体に含浸させる工程と、第1の重合性成分を、第1の重合開始剤により重合させる工程と、を備える、半硬化物複合体の製造方法を提供する。【選択図】なし
PRODUCTION METHOD OF SEMI-CURED COMPOSITE, METHOD FOR PRODUCING CURED COMPOSITE, AND SEMI-CURED COMPOSITE
半硬化物複合体の製造方法、硬化物複合体の製造方法、及び半硬化物複合体
KANEKO ERI (Autor:in) / INOUE SAORI (Autor:in) / TSUJI KOJI (Autor:in)
28.03.2023
Patent
Elektronische Ressource
Japanisch
IPC:
C04B
Kalk
,
LIME
Europäisches Patentamt | 2022
|METHOD FOR PRODUCING CURED GEOPOLYMER, AND CURED GEOPOLYMER
Europäisches Patentamt | 2024
|KIT FOR PREPARING CURED PRODUCT, METHOD FOR PRODUCING CURED PRODUCT AND CURED PRODUCT
Europäisches Patentamt | 2022
|