ADDITIVE FOR POLYMER MODIFIED ASPHALT POLYMER MODIFIED ASPHALT COMPOSITION COMPRISING THE SAME AND METHOD FOR PREPARING THE SAME
An embodiment of the present invention provides a manufacturing method of an additive for modified asphalt, which comprises: a step (a) of adding a conjugated diene monomer, an organometallic catalyst, and a solvent to a reactor for reaction; and a step (b) of preparing a copolymer represented by chemical formula 1, A-B-C, and having a weight average molecular weight (M_w) of 140,000 g/mol or less by adding an aromatic vinyl monomer and a randomizing agent to the reactor in a section, in which the polymerization conversion rate of the conjugated diene monomer is 40 to 95%, and reacting the same. In chemical formula 1, A is a first block made of a conjugated diene monomer, B is a second block made of a conjugated diene monomer and an aromatic vinyl monomer, C is a third block made of an aromatic vinyl monomer. The content of the aromatic vinyl monomer included in C is 60 to 90 wt% based on the total weight of the aromatic vinyl monomer included in the copolymer. Accordingly, the present invention can provide the manufacturing method of an economical additive for modified asphalt with excellent performance.
본 발명의 일 실시예는 (a) 반응기에 공액 디엔 단량체, 유기금속촉매 및 용매를 투입하여 반응시키는 단계; 및 (b) 상기 공액 디엔 단량체의 중합 전환율이 40~95%인 구간에서 상기 반응기에 방향족 비닐 단량체 및 랜덤화제를 투입하여 반응시켜 하기 화학식 1로 표시되고 중량평균분자량(M)이 140,000g/mol 이하인 공중합체를 제조하는 단계;를 포함하는, 개질 아스팔트용 첨가제의 제조방법을 제공한다. <화학식 1> A-B-C 상기 화학식 1에서, A는 공액 디엔 단량체로 이루어진 제1 블록이고, B는 공액 디엔 단량체 및 방향족 비닐 단량체로 이루어진 제2 블록이고, C는 방향족 비닐 단량체로 이루어진 제3 블록이고, 상기 공중합체에 포함된 방향족 비닐 단량체의 총 중량을 기준으로 상기 C에 포함된 방향족 비닐 단량체의 함량은 60~90중량%이다.
ADDITIVE FOR POLYMER MODIFIED ASPHALT POLYMER MODIFIED ASPHALT COMPOSITION COMPRISING THE SAME AND METHOD FOR PREPARING THE SAME
An embodiment of the present invention provides a manufacturing method of an additive for modified asphalt, which comprises: a step (a) of adding a conjugated diene monomer, an organometallic catalyst, and a solvent to a reactor for reaction; and a step (b) of preparing a copolymer represented by chemical formula 1, A-B-C, and having a weight average molecular weight (M_w) of 140,000 g/mol or less by adding an aromatic vinyl monomer and a randomizing agent to the reactor in a section, in which the polymerization conversion rate of the conjugated diene monomer is 40 to 95%, and reacting the same. In chemical formula 1, A is a first block made of a conjugated diene monomer, B is a second block made of a conjugated diene monomer and an aromatic vinyl monomer, C is a third block made of an aromatic vinyl monomer. The content of the aromatic vinyl monomer included in C is 60 to 90 wt% based on the total weight of the aromatic vinyl monomer included in the copolymer. Accordingly, the present invention can provide the manufacturing method of an economical additive for modified asphalt with excellent performance.
본 발명의 일 실시예는 (a) 반응기에 공액 디엔 단량체, 유기금속촉매 및 용매를 투입하여 반응시키는 단계; 및 (b) 상기 공액 디엔 단량체의 중합 전환율이 40~95%인 구간에서 상기 반응기에 방향족 비닐 단량체 및 랜덤화제를 투입하여 반응시켜 하기 화학식 1로 표시되고 중량평균분자량(M)이 140,000g/mol 이하인 공중합체를 제조하는 단계;를 포함하는, 개질 아스팔트용 첨가제의 제조방법을 제공한다. <화학식 1> A-B-C 상기 화학식 1에서, A는 공액 디엔 단량체로 이루어진 제1 블록이고, B는 공액 디엔 단량체 및 방향족 비닐 단량체로 이루어진 제2 블록이고, C는 방향족 비닐 단량체로 이루어진 제3 블록이고, 상기 공중합체에 포함된 방향족 비닐 단량체의 총 중량을 기준으로 상기 C에 포함된 방향족 비닐 단량체의 함량은 60~90중량%이다.
ADDITIVE FOR POLYMER MODIFIED ASPHALT POLYMER MODIFIED ASPHALT COMPOSITION COMPRISING THE SAME AND METHOD FOR PREPARING THE SAME
개질 아스팔트용 첨가제, 이를 포함하는 개질 아스팔트 조성물 및 그 제조방법
NOH EUN KYUNG (Autor:in) / CHEEN SUN WOO (Autor:in) / PARK HAN SOO (Autor:in) / KO JAE YOUNG (Autor:in)
30.09.2019
Patent
Elektronische Ressource
Koreanisch
Europäisches Patentamt | 2017
|Europäisches Patentamt | 2020
|Europäisches Patentamt | 2020
Europäisches Patentamt | 2024
|MODIFIED ASPHALT BINDER COMPOSITION AND MODIFIED ASPHALT MIXTURE COMPRISING THE SAME
Europäisches Patentamt | 2023
|