Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
MULTI LAYER ASPHALT CONSTRUCTION METHOD
The present invention relates to a multi-layered asphalt composition and a construction method thereof, which is to improve constructability and shorten a construction period by packaging a surface layer and a base layer at the same time during an asphalt paving work. To this end, the multi-layered asphalt composition of the present invention has a surface layer including a drainage asphalt composition, formed of upper and lower layers. The upper layer has a composition of 70 to 90 wt% of coarse aggregate having a particle diameter of 4 to 10 mm, 1 to 20 wt% of fine aggregate having a particle diameter of 0.1 to 4 mm, 3 to 12 wt% of limestone powder, 0.1 to 1 wt% of a vegetable fiber additive, 4 to 12 wt% of an asphalt binder, and 0.3 to 1.5 wt% of an asphalt modifier. Also, the lower layer includes 73 to 93 wt% of coarse aggregate having a particle diameter of 8 to 20 mm, 1 to 15 wt% of fine aggregate having a particle diameter of 0.1 to 8 mm, 1 to 10 wt% of limestone powder, 0.1 to 1 wt% of a vegetable fiber additive, 4 to 12 wt% of an asphalt binder, and 0.3 to 1.5 wt% of an asphalt modifier.
본 발명은 복층 아스팔트 조성물 및 시공방법에 관한 것으로서, 아스팔트 포장작업시 표층과 기층을 동시에 포장함으로서 시공성을 향상시킴과 함께 공사기간을 단축할 수 있는 효과를 나타내기 위한 것이다. 이를 실현하기 위한 본 발명은, 배수성 아스팔트 조성물로 이루어지는 표층이 상부층과 하부층의 복층으로 이루어지는 복층 아스팔트 조성물에 있어서, 상기 상부층은, 입경 4~10mm의 굵은골재 70~90중량%, 입경 0.1~4mm의 잔골재 1~20중량%, 석회석분 3~12중량%, 식물성 섬유첨가재 0.1~1중량%, 아스팔트 바인더 4~12중량%, 아스팔트 개질제 0.3~1.5중량%의 조성을 이루고, 상기 하부층은, 입경 8~20mm의 굵은골재 73~93중량%, 입경 0.1~8mm의 잔골재 1~15중량%, 석회석분 1~10중량%, 식물성 섬유첨가재 0.1~1중량%, 아스팔트 바인더 4~12중량%, 아스팔트 개질제 0.3~1.5중량%의 조성을 이루는 것을 특징으로 한다.
MULTI LAYER ASPHALT CONSTRUCTION METHOD
The present invention relates to a multi-layered asphalt composition and a construction method thereof, which is to improve constructability and shorten a construction period by packaging a surface layer and a base layer at the same time during an asphalt paving work. To this end, the multi-layered asphalt composition of the present invention has a surface layer including a drainage asphalt composition, formed of upper and lower layers. The upper layer has a composition of 70 to 90 wt% of coarse aggregate having a particle diameter of 4 to 10 mm, 1 to 20 wt% of fine aggregate having a particle diameter of 0.1 to 4 mm, 3 to 12 wt% of limestone powder, 0.1 to 1 wt% of a vegetable fiber additive, 4 to 12 wt% of an asphalt binder, and 0.3 to 1.5 wt% of an asphalt modifier. Also, the lower layer includes 73 to 93 wt% of coarse aggregate having a particle diameter of 8 to 20 mm, 1 to 15 wt% of fine aggregate having a particle diameter of 0.1 to 8 mm, 1 to 10 wt% of limestone powder, 0.1 to 1 wt% of a vegetable fiber additive, 4 to 12 wt% of an asphalt binder, and 0.3 to 1.5 wt% of an asphalt modifier.
본 발명은 복층 아스팔트 조성물 및 시공방법에 관한 것으로서, 아스팔트 포장작업시 표층과 기층을 동시에 포장함으로서 시공성을 향상시킴과 함께 공사기간을 단축할 수 있는 효과를 나타내기 위한 것이다. 이를 실현하기 위한 본 발명은, 배수성 아스팔트 조성물로 이루어지는 표층이 상부층과 하부층의 복층으로 이루어지는 복층 아스팔트 조성물에 있어서, 상기 상부층은, 입경 4~10mm의 굵은골재 70~90중량%, 입경 0.1~4mm의 잔골재 1~20중량%, 석회석분 3~12중량%, 식물성 섬유첨가재 0.1~1중량%, 아스팔트 바인더 4~12중량%, 아스팔트 개질제 0.3~1.5중량%의 조성을 이루고, 상기 하부층은, 입경 8~20mm의 굵은골재 73~93중량%, 입경 0.1~8mm의 잔골재 1~15중량%, 석회석분 1~10중량%, 식물성 섬유첨가재 0.1~1중량%, 아스팔트 바인더 4~12중량%, 아스팔트 개질제 0.3~1.5중량%의 조성을 이루는 것을 특징으로 한다.
MULTI LAYER ASPHALT CONSTRUCTION METHOD
복층 아스팔트 시공방법
KIM BYEONG CHAE (Autor:in) / WOO JUN JE (Autor:in) / KIM JAE WON (Autor:in) / KIM HYEON JIN (Autor:in) / LEE MOON SUP (Autor:in) / JEON SUNG IL (Autor:in) / KWON SOO AHN (Autor:in) / NOH JAE MYEON (Autor:in) / SON JEONG TAN (Autor:in) / HAN YEONG NAM (Autor:in)
16.07.2019
Patent
Elektronische Ressource
Koreanisch
Construction method of asphalt waterproof paint layer
Europäisches Patentamt | 2020
|Construction method of stress absorption layer asphalt pavement
Europäisches Patentamt | 2021
|Construction method of asphalt mastic upper surface layer
Europäisches Patentamt | 2024
|