Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Low cement-based solidification agent composition for solidifying weak ground and method for solidifying weak ground using the same
The present invention relates to a low cement-based solidification agent composition for solidifying a weak ground and a method for treating the weak ground using the same. The low cement-based solidification agent composition includes: 10 to 25 wt% of pulverized coal boiler fly ash; 7 to 25 wt% of fluid bed boiler fly ash; 10 to 25 wt% of paper sludge incineration ash; 5 to 35 wt% of at least one slag selected from the group consisting of blast furnace slag, ferronickel slag, coal gasification composite slag, and mixed slag thereof; 5 to 10 wt% of gypsum; 5 to 30 wt% of at least one cement selected from the group consisting of general Portland cement, crude steel cement, ultrafast-cured cement, CSA-based cement, and mixtures thereof; 1 to 7 wt% of bentonite; 0.01 to 0.2 wt% of retarder; 0.01 to 0.2 wt% of a curing accelerator; and 0.01 to 0.2 wt% of admixture. Therefore, it is eco-friendly and has improved physical properties by utilizing recycled resources (industrial by-products) generated in the industry and minimizing the used amount of cement.
본 발명은 미분탄 보일러 플라이애시 10 내지 25 중량%; 유동층 보일러 플라이애시 7 내지 25 중량%; 제지슬러지 소각재 10 내지 25 중량%; 고로슬래그, 페로니켈 슬래그, 석탄가스화 복합슬래그 및 이들의 혼합 슬래그로 이루어진 군에서 선택되는 1종 이상의 슬래그 5 내지 35 중량%; 석고 5 내지 10 중량%; 보통 포틀랜드 시멘트, 조강 시멘트, 초속경 시멘트, CSA계 시멘트 및 이들의 혼합물로 이루어진 군에서 선택되는 1종 이상의 시멘트 5 내지 30 중량%; 벤토나이트 1 내지 7 중량%; 지연제 0.01 내지 0.2 중량%; 경화 촉진제 0.01 내지 0.2 중량%; 및 혼화제 0.01 내지 0.2 중량%;를 포함하여, 산업계에서 발생되는 순환자원(산업 부산물)을 활용하고 시멘트 사용량을 최소화하여 친환경적인 동시에 개선된 물리적 특성을 갖는 저시멘트계 연약지반 강화용 고화재 조성물 및 이를 이용한 연약지반 처리공법에 관한 것이다.
Low cement-based solidification agent composition for solidifying weak ground and method for solidifying weak ground using the same
The present invention relates to a low cement-based solidification agent composition for solidifying a weak ground and a method for treating the weak ground using the same. The low cement-based solidification agent composition includes: 10 to 25 wt% of pulverized coal boiler fly ash; 7 to 25 wt% of fluid bed boiler fly ash; 10 to 25 wt% of paper sludge incineration ash; 5 to 35 wt% of at least one slag selected from the group consisting of blast furnace slag, ferronickel slag, coal gasification composite slag, and mixed slag thereof; 5 to 10 wt% of gypsum; 5 to 30 wt% of at least one cement selected from the group consisting of general Portland cement, crude steel cement, ultrafast-cured cement, CSA-based cement, and mixtures thereof; 1 to 7 wt% of bentonite; 0.01 to 0.2 wt% of retarder; 0.01 to 0.2 wt% of a curing accelerator; and 0.01 to 0.2 wt% of admixture. Therefore, it is eco-friendly and has improved physical properties by utilizing recycled resources (industrial by-products) generated in the industry and minimizing the used amount of cement.
본 발명은 미분탄 보일러 플라이애시 10 내지 25 중량%; 유동층 보일러 플라이애시 7 내지 25 중량%; 제지슬러지 소각재 10 내지 25 중량%; 고로슬래그, 페로니켈 슬래그, 석탄가스화 복합슬래그 및 이들의 혼합 슬래그로 이루어진 군에서 선택되는 1종 이상의 슬래그 5 내지 35 중량%; 석고 5 내지 10 중량%; 보통 포틀랜드 시멘트, 조강 시멘트, 초속경 시멘트, CSA계 시멘트 및 이들의 혼합물로 이루어진 군에서 선택되는 1종 이상의 시멘트 5 내지 30 중량%; 벤토나이트 1 내지 7 중량%; 지연제 0.01 내지 0.2 중량%; 경화 촉진제 0.01 내지 0.2 중량%; 및 혼화제 0.01 내지 0.2 중량%;를 포함하여, 산업계에서 발생되는 순환자원(산업 부산물)을 활용하고 시멘트 사용량을 최소화하여 친환경적인 동시에 개선된 물리적 특성을 갖는 저시멘트계 연약지반 강화용 고화재 조성물 및 이를 이용한 연약지반 처리공법에 관한 것이다.
Low cement-based solidification agent composition for solidifying weak ground and method for solidifying weak ground using the same
저시멘트계 연약지반 강화용 고화재 조성물 및 이를 이용한 연약지반 처리공법
WOO YANG YI (Autor:in) / PARK KEUN BAE (Autor:in) / CHO NAM WOO (Autor:in)
02.06.2020
Patent
Elektronische Ressource
Koreanisch
Europäisches Patentamt | 2020
|GROUND SOLIDIFYING AGENT, PRODUCTION METHOD AND GROUND SOLIDIFYING METHOD
Europäisches Patentamt | 2018
|Europäisches Patentamt | 2022
|Europäisches Patentamt | 2017
|