AQUATIC HARDENING MORTAR COMPOSITION AND REPAIR-REINFORCEMENT METHOD USING THE SAME
The present invention relates to an underwater hardening mortar composition, and a repairing and reinforcing method for an underwater concrete structure using the same. The underwater hardening mortar composition comprises 20 to 40 wt% of cement, 5 to 20 wt% of a superhydrophobic hardening agent in which at least one adhesive selected from the group consisting of epoxy, polyurethane, and acryl urethane, and silica aerogel of nano-sized particles are dispersed in a weight ratio of 5:1 to 1:1, 3 to 15 wt% of an expansion agent, 5 to 20 wt% of a filler, 20 to 55 wt% of particle size-adjusting silica sand, 0.2 to 1 wt% of a fluidizing agent selected from the group consisting of melamine-based, naphthalene-based, and carboxyl-based fluidizing agents, 0.05 to 2 wt% of a reactivity-adjusting agent, and 0.2 to 3 wt% of a stabilizer consisting of at least one of calcium-based, barium-based, zinc-based, and magnesium-based stearate. The repairing and reinforcing method for an underwater concrete structure comprises: a preparation step of excavating the lowest part of the periphery of the underwater concrete structure and cleaning a part to be repaired at a high pressure; a step of installing a reinforcing frame to be spaced apart from the outer surface of the underwater concrete structure at a predetermined interval; a pouring step of filling the part to be repaired by injecting underwater hardening mortar into a space between the underwater concrete structure and the reinforcing frame; and a finishing step of filling an excavated part of the periphery of the underwater concrete structure in which the reinforcing frame is installed, with the underwater hardening mortar and hardening the underwater hardening mortar. According to the present invention, the lifetime of an underwater concrete structure can be extended.
본 발명은 수중경화몰탈 조성물 및 이를 이용한 수중 콘크리트 구조물의 보수보강공법에 관한 것으로서, 구체적으로 수중경화몰탈 조성물은 시멘트 20 내지 40wt%, 에폭시, 폴리우레탄, 아크릴우레탄으로 이루어진 군에서 선택된 어느 하나 이상의 접착제와 나노크기 입자의 실리카 에어로겔이 5:1~1:1 의 중량비로 분산된 초발수 경화제 5 내지 20wt%, 팽창재 3 내지 15wt%, 충진재 5 내지 20wt%, 입도 조정 규사 20 내지 55wt%, 멜라민계, 나프탈렌계, 카르복실계 유동화제로 이루어진 군에서 선택된 어느 하나의 유동화제 0.2 내지 1wt%, 반응성 조절제 0.05 내지 2wt%, 및 칼슘계, 바륨계, 아연계, 및 마그네슘계 스테아린산염 중 어느 하나 이상으로 이루어진 안정제 0.2 내지 3wt%을 포함하고, 수중 콘크리트 구조물의 보수보강공법은 수중 콘크리트 구조물의 수중 최저 주변부에 터파기를 하고, 보수 대상부위를 고압 세척하는 준비 단계, 수중 콘크리트 구조물 외부면을 따라 소정의 간격으로 이격된 보강틀을 설치하는 단계, 상기 수중 콘크리트 구조물과 보강틀 사이의 이격 공간으로 수중경화몰탈을 주입하여 상기 보수 대상부위를 충진시키는 타설 단계, 및 보강틀이 설치된 콘크리트 구조물의 주변부의 터파기 부위에 상기 수중경화몰탈을 채워 경화시키는 마감 단계를 포함한다.
AQUATIC HARDENING MORTAR COMPOSITION AND REPAIR-REINFORCEMENT METHOD USING THE SAME
The present invention relates to an underwater hardening mortar composition, and a repairing and reinforcing method for an underwater concrete structure using the same. The underwater hardening mortar composition comprises 20 to 40 wt% of cement, 5 to 20 wt% of a superhydrophobic hardening agent in which at least one adhesive selected from the group consisting of epoxy, polyurethane, and acryl urethane, and silica aerogel of nano-sized particles are dispersed in a weight ratio of 5:1 to 1:1, 3 to 15 wt% of an expansion agent, 5 to 20 wt% of a filler, 20 to 55 wt% of particle size-adjusting silica sand, 0.2 to 1 wt% of a fluidizing agent selected from the group consisting of melamine-based, naphthalene-based, and carboxyl-based fluidizing agents, 0.05 to 2 wt% of a reactivity-adjusting agent, and 0.2 to 3 wt% of a stabilizer consisting of at least one of calcium-based, barium-based, zinc-based, and magnesium-based stearate. The repairing and reinforcing method for an underwater concrete structure comprises: a preparation step of excavating the lowest part of the periphery of the underwater concrete structure and cleaning a part to be repaired at a high pressure; a step of installing a reinforcing frame to be spaced apart from the outer surface of the underwater concrete structure at a predetermined interval; a pouring step of filling the part to be repaired by injecting underwater hardening mortar into a space between the underwater concrete structure and the reinforcing frame; and a finishing step of filling an excavated part of the periphery of the underwater concrete structure in which the reinforcing frame is installed, with the underwater hardening mortar and hardening the underwater hardening mortar. According to the present invention, the lifetime of an underwater concrete structure can be extended.
본 발명은 수중경화몰탈 조성물 및 이를 이용한 수중 콘크리트 구조물의 보수보강공법에 관한 것으로서, 구체적으로 수중경화몰탈 조성물은 시멘트 20 내지 40wt%, 에폭시, 폴리우레탄, 아크릴우레탄으로 이루어진 군에서 선택된 어느 하나 이상의 접착제와 나노크기 입자의 실리카 에어로겔이 5:1~1:1 의 중량비로 분산된 초발수 경화제 5 내지 20wt%, 팽창재 3 내지 15wt%, 충진재 5 내지 20wt%, 입도 조정 규사 20 내지 55wt%, 멜라민계, 나프탈렌계, 카르복실계 유동화제로 이루어진 군에서 선택된 어느 하나의 유동화제 0.2 내지 1wt%, 반응성 조절제 0.05 내지 2wt%, 및 칼슘계, 바륨계, 아연계, 및 마그네슘계 스테아린산염 중 어느 하나 이상으로 이루어진 안정제 0.2 내지 3wt%을 포함하고, 수중 콘크리트 구조물의 보수보강공법은 수중 콘크리트 구조물의 수중 최저 주변부에 터파기를 하고, 보수 대상부위를 고압 세척하는 준비 단계, 수중 콘크리트 구조물 외부면을 따라 소정의 간격으로 이격된 보강틀을 설치하는 단계, 상기 수중 콘크리트 구조물과 보강틀 사이의 이격 공간으로 수중경화몰탈을 주입하여 상기 보수 대상부위를 충진시키는 타설 단계, 및 보강틀이 설치된 콘크리트 구조물의 주변부의 터파기 부위에 상기 수중경화몰탈을 채워 경화시키는 마감 단계를 포함한다.
AQUATIC HARDENING MORTAR COMPOSITION AND REPAIR-REINFORCEMENT METHOD USING THE SAME
수중경화몰탈 조성물 및 이를 이용한 보수보강공법
JUNG SI YOUNG (Autor:in)
23.02.2021
Patent
Elektronische Ressource
Koreanisch
IPC:
C04B
Kalk
,
LIME
Europäisches Patentamt | 2022
|REPAIR MORTAR MATERIAL, REPAIR MORTAR COMPOSITION, AND HARDENING BODY
Europäisches Patentamt | 2022
|Quick-hardening repair mortar material, quick-hardening repair mortar composition, and hardened body
Europäisches Patentamt | 2023
|