Concrete composition for precast concrete
The present invention relates to a crude steel admixture for improving the strength of precast concrete (PC), securing early strength, and reducing drying shrinkage and a binder composition and a concrete composition containing the same. The present invention provides a crude steel admixture for PC, which comprises: 20 to 80 wt% of blast furnace slag fine powder; 10 to 60 wt% of desulfurized gypsum; and 1 to 20 wt% of STS converter slag. In addition, the present invention also provides a binder composition for PC, which comprises: 70 to 80 wt% of one kind of ordinary Portland cement; and 20 to 30 wt% of a crude steel admixture for PC, and a concrete composition for PC, which comprises: 430 to 480 kg/㎥ of the binder composition for PC; and 700 to 750 kg/㎥ of fine aggregate under the conditions of 40 to 45 vol% of an aggregate ratio, 33 to 38 wt% of a water-to-binder ratio, and 0.8 to 1.0 wt% of a water reducing agent-to-the binder composition.
본 발명은 프리캐스트 콘크리트의 강도 증진, 조기강도 확보 및 건조수축 저감을 위한 조강 혼화재 및 이를 포함하는 결합재 조성물과 콘크리트 조성물에 관한 것이다. 본 발명은 「고로슬래그 미분말 20~80 wt%; 탈황석고 10~60 wt%; 및 STS 전로슬래그 1~20 wt%; 를 포함하는 PC용 조강 혼화재」를 제공한다. 또한, 본 발명은 「1종 보통포틀랜드시멘트 70~80 wt%; 및 상기 PC용 조강 혼화재 20~30 wt%; 를 포함하는 PC용 결합재 조성물」과, 「상기 PC용 결합재 조성물 430~480 kg/㎥; 잔골재 700~750 kg/㎥; 잔골재율 40~45 vol%; 물/결합재비 33~38 wt%; 상기 결합재 조성물 대비 감수제 0.8~1.0 wt%; 조건으로 배합된 PC용 콘크리트 조성물」을 함께 제공한다.
Concrete composition for precast concrete
The present invention relates to a crude steel admixture for improving the strength of precast concrete (PC), securing early strength, and reducing drying shrinkage and a binder composition and a concrete composition containing the same. The present invention provides a crude steel admixture for PC, which comprises: 20 to 80 wt% of blast furnace slag fine powder; 10 to 60 wt% of desulfurized gypsum; and 1 to 20 wt% of STS converter slag. In addition, the present invention also provides a binder composition for PC, which comprises: 70 to 80 wt% of one kind of ordinary Portland cement; and 20 to 30 wt% of a crude steel admixture for PC, and a concrete composition for PC, which comprises: 430 to 480 kg/㎥ of the binder composition for PC; and 700 to 750 kg/㎥ of fine aggregate under the conditions of 40 to 45 vol% of an aggregate ratio, 33 to 38 wt% of a water-to-binder ratio, and 0.8 to 1.0 wt% of a water reducing agent-to-the binder composition.
본 발명은 프리캐스트 콘크리트의 강도 증진, 조기강도 확보 및 건조수축 저감을 위한 조강 혼화재 및 이를 포함하는 결합재 조성물과 콘크리트 조성물에 관한 것이다. 본 발명은 「고로슬래그 미분말 20~80 wt%; 탈황석고 10~60 wt%; 및 STS 전로슬래그 1~20 wt%; 를 포함하는 PC용 조강 혼화재」를 제공한다. 또한, 본 발명은 「1종 보통포틀랜드시멘트 70~80 wt%; 및 상기 PC용 조강 혼화재 20~30 wt%; 를 포함하는 PC용 결합재 조성물」과, 「상기 PC용 결합재 조성물 430~480 kg/㎥; 잔골재 700~750 kg/㎥; 잔골재율 40~45 vol%; 물/결합재비 33~38 wt%; 상기 결합재 조성물 대비 감수제 0.8~1.0 wt%; 조건으로 배합된 PC용 콘크리트 조성물」을 함께 제공한다.
Concrete composition for precast concrete
PC용 콘크리트 조성물
KIM YEONOK (Autor:in) / HWANG SUNKYUNG (Autor:in) / SHIN KYOUNGSU (Autor:in) / KIM HYUNJUN (Autor:in) / HEO SEONGYEONG (Autor:in)
28.04.2023
Patent
Elektronische Ressource
Koreanisch
IPC:
C04B
Kalk
,
LIME
Precast Concrete Member Manufacturing Method Using Self-leveling Precast Concrete Composition
Europäisches Patentamt | 2020
|PRECAST - Precast Concrete Frames
Online Contents | 1998
|PRECAST CONCRETE - Precast concrete floors: The future
Online Contents | 2001
|