Eine Plattform für die Wissenschaft: Bauingenieurwesen, Architektur und Urbanistik
Block for reducing heat island phenomenon using surface-modified waste glass aggregate
본 발명은 열전달률이 낮으며 골재-매트릭스 간 슬립 현상을 저감시킬 수 있도록 표면에 C-S-H 결정질이 코팅된 표면 개질 폐유리골재 및 보수성을 가진 왕겨를 활용하여 친환경적, 경량성, 투수성 및 보수성을 함께 확보할 수 있는 열섬 저감 블록에 관한 것이다. 본 발명은 「입경 3~5mm의 폐유리골재 40~50vol%; 입경 3~10mm의 폐블록 파쇄물 20~35vol%; 왕겨 3~7vol%; 고로슬래그 시멘트계 무기결합재 10~15vol%; 및 물 6~12vol%; 를 혼합한 조성물을 형틀에 넣고 압착시켜 제조한 투수성과 보수성을 함께 구비한 표면 개질 폐유리골재를 활용한 열섬 저감 블록」을 제공한다.
The present invention relates to a heat island reduction block which is eco-friendly, lightweight, water permeable, and water retentive by using a surface-modified waste glass aggregate with a C-S-H crystalline coating on the surface to reduce the heat transfer rate and the aggregate-matrix slip phenomenon, and by using chaff with water retention properties. The present invention provides the heat island reduction block using surface-modified waste glass aggregate with water permeability and water retention, which is manufactured by pressing, in a mold, a composition comprising 40-50 vol% of waste glass aggregate with a diameter of 3-5 mm; 20-35 vol% of waste block crushed material with a diameter of 3-10 mm; 3-7 vol% of chaff; 10-15 vol% of blast furnace slag cement-based inorganic binder; and 6-12 vol% of water.
Block for reducing heat island phenomenon using surface-modified waste glass aggregate
본 발명은 열전달률이 낮으며 골재-매트릭스 간 슬립 현상을 저감시킬 수 있도록 표면에 C-S-H 결정질이 코팅된 표면 개질 폐유리골재 및 보수성을 가진 왕겨를 활용하여 친환경적, 경량성, 투수성 및 보수성을 함께 확보할 수 있는 열섬 저감 블록에 관한 것이다. 본 발명은 「입경 3~5mm의 폐유리골재 40~50vol%; 입경 3~10mm의 폐블록 파쇄물 20~35vol%; 왕겨 3~7vol%; 고로슬래그 시멘트계 무기결합재 10~15vol%; 및 물 6~12vol%; 를 혼합한 조성물을 형틀에 넣고 압착시켜 제조한 투수성과 보수성을 함께 구비한 표면 개질 폐유리골재를 활용한 열섬 저감 블록」을 제공한다.
The present invention relates to a heat island reduction block which is eco-friendly, lightweight, water permeable, and water retentive by using a surface-modified waste glass aggregate with a C-S-H crystalline coating on the surface to reduce the heat transfer rate and the aggregate-matrix slip phenomenon, and by using chaff with water retention properties. The present invention provides the heat island reduction block using surface-modified waste glass aggregate with water permeability and water retention, which is manufactured by pressing, in a mold, a composition comprising 40-50 vol% of waste glass aggregate with a diameter of 3-5 mm; 20-35 vol% of waste block crushed material with a diameter of 3-10 mm; 3-7 vol% of chaff; 10-15 vol% of blast furnace slag cement-based inorganic binder; and 6-12 vol% of water.
Block for reducing heat island phenomenon using surface-modified waste glass aggregate
표면 개질 폐유리골재를 활용한 열섬 저감 블록
18.04.2024
Patent
Elektronische Ressource
Koreanisch
IPC:
C04B
Kalk
,
LIME
/
B28B
Formgeben von Ton oder anderen keramischen Stoffzusammensetzungen, Schlacke oder von Mischungen, die zementartiges Material enthalten, z.B. Putzmörtel
,
SHAPING CLAY OR OTHER CERAMIC COMPOSITIONS, SLAG OR MIXTURES CONTAINING CEMENTITIOUS MATERIAL, e.g. PLASTER
/
E01C
Bau von Straßen, Sportplätzen oder dgl., Decken dafür
,
CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, OR THE LIKE
Block for reducing heat island phenomenon using surface-modified waste glass aggregate
Europäisches Patentamt | 2023
|Waste glass fine aggregate surface modification method Surface modified waste glass fine aggregate
Europäisches Patentamt | 2022
|Reducing heat island effect by using recycled glass cullet in asphalt shingles
BASE | 2015
|Europäisches Patentamt | 2024
|Influence of heat island phenomenon on building heat load
British Library Online Contents | 2002
|