Flowable Fill
The present invention relates to liquefied stabilized soil for filling and, more specifically, includes 30 to 70% by weight of ferronickel slag, 5 to 30% by weight of in situ soil, 5 to 10% by weight of cementitious solidifying material, and 10 to 30% by weight of coal ash. According to the liquefied stabilized soil for filling of the present invention, by recycling and using ferronickel slag and in situ soil as the main raw material of the liquefied stabilized soil for filling, the liquefied stabilized soil for filling has the same level of fluidity and compressive strength of the existing liquefied stabilized soil for filling, while the waste of resources can be significantly reduced, and pollution to the soil can be minimized. In addition, since the liquefied stabilized soil for filling of the present invention contains waste tire rubber powder, it is possible to suppress cracks caused by drying shrinkage that occur during the curing period after construction.
본 발명은 채움용 유동화토에 관한 것으로, 보다 구체적으로 페로니켈슬래그 30 내지 70 중량%, 현장발생토 5 내지 30 중량%, 시멘트계 고화재 5 내지 10 중량% 및 석탄회 10 내지 30 중량%를 포함한다. 본 발명의 채움용 유동화토에 의하면, 페로니켈슬래그와 현장발생토를 채움용 유동화토의 주원료로 재활용하여 사용함으로써, 기존의 채움용 유동화토가 가지는 유동성 및 압축강도는 동등 수준으로 갖추면서, 자원의 낭비는 현저히 줄일 수 있고, 토양에 대한 오염은 최소화할 수 있는 효과가 있다. 또한, 본 발명의 채움용 유동화토는 폐타이어 고무 분말을 함유함으로써, 시공 후 양생기간 중 발생하는 건조수축에 의한 균열을 억제할 수 있는 효과가 있다.
Flowable Fill
The present invention relates to liquefied stabilized soil for filling and, more specifically, includes 30 to 70% by weight of ferronickel slag, 5 to 30% by weight of in situ soil, 5 to 10% by weight of cementitious solidifying material, and 10 to 30% by weight of coal ash. According to the liquefied stabilized soil for filling of the present invention, by recycling and using ferronickel slag and in situ soil as the main raw material of the liquefied stabilized soil for filling, the liquefied stabilized soil for filling has the same level of fluidity and compressive strength of the existing liquefied stabilized soil for filling, while the waste of resources can be significantly reduced, and pollution to the soil can be minimized. In addition, since the liquefied stabilized soil for filling of the present invention contains waste tire rubber powder, it is possible to suppress cracks caused by drying shrinkage that occur during the curing period after construction.
본 발명은 채움용 유동화토에 관한 것으로, 보다 구체적으로 페로니켈슬래그 30 내지 70 중량%, 현장발생토 5 내지 30 중량%, 시멘트계 고화재 5 내지 10 중량% 및 석탄회 10 내지 30 중량%를 포함한다. 본 발명의 채움용 유동화토에 의하면, 페로니켈슬래그와 현장발생토를 채움용 유동화토의 주원료로 재활용하여 사용함으로써, 기존의 채움용 유동화토가 가지는 유동성 및 압축강도는 동등 수준으로 갖추면서, 자원의 낭비는 현저히 줄일 수 있고, 토양에 대한 오염은 최소화할 수 있는 효과가 있다. 또한, 본 발명의 채움용 유동화토는 폐타이어 고무 분말을 함유함으로써, 시공 후 양생기간 중 발생하는 건조수축에 의한 균열을 억제할 수 있는 효과가 있다.
Flowable Fill
채움용 유동화토
30.11.2021
Patent
Elektronische Ressource
Koreanisch
British Library Conference Proceedings | 1997
|Flowable Fill Using Waste Products
British Library Conference Proceedings | 1996
|