SETTABLE COMPOSITIONS CONTAINING NON-EXPANDED PEARLITE (VERSIONS)
FIELD: construction.SUBSTANCE: implementation version of the present invention includes a settable composition containing ground non-expanded pearlite, pumicite, cement kiln dust, and water. Another implementation version of the present invention includes a settable composition containing ground non-expanded pearlite present in an amount of from about 1% to about 75% of the weight of the cementing components in the settable composition, the ground non-expanded pearlite having an average particle size from about 1 mcm to about 100 mcm, cement kiln dust, the ground mixture of cement and pumicite, and water. Another implementation version of the present invention includes a settable composition containing ground non-expanded pearlite present in an amount of from about 1% to about 75% of the weight of the cementing components in the settable composition, cement kiln dust, pumicite, and functional additives. The invention is developed in the dependent claims of the invention formula.EFFECT: increased efficiency of cementing.20 cl, 6 tbl, 6 ex
Изобретение относится к операциям цементирования. Вариант осуществления настоящего изобретения включает способную к схватыванию композицию, содержащую размолотый невспученный перлит, пумицит, цементную печную пыль и воду. Другой вариант осуществления настоящего изобретения включает способную к схватыванию композицию, содержащую размолотый невспученный перлит, присутствующий в количестве от примерно 1% до примерно 75% от массы цементирующих компонентов в способной к схватыванию композиции, причем размолотый невспученный перлит имеет средний размер частиц от примерно 1 мкм до примерно 100 мкм, цементную печную пыль, размолотую смесь цемента и пумицита и воду. Еще один вариант осуществления настоящего изобретения включает способную к схватыванию композицию, содержащую размолотый невспученный перлит, присутствующий в количестве от примерно 1% до примерно 75% от массы цементирующих компонентов в способной к схватыванию композиции, цементную печную пыль, пумицит и функциональные добавки. Изобретение развито в зависимых пунктах формулы изобретения. Технический результат - повышение эффективности цементирования. 3 н. и 17 з.п. ф-лы, 6 табл., 6 пр.
SETTABLE COMPOSITIONS CONTAINING NON-EXPANDED PEARLITE (VERSIONS)
FIELD: construction.SUBSTANCE: implementation version of the present invention includes a settable composition containing ground non-expanded pearlite, pumicite, cement kiln dust, and water. Another implementation version of the present invention includes a settable composition containing ground non-expanded pearlite present in an amount of from about 1% to about 75% of the weight of the cementing components in the settable composition, the ground non-expanded pearlite having an average particle size from about 1 mcm to about 100 mcm, cement kiln dust, the ground mixture of cement and pumicite, and water. Another implementation version of the present invention includes a settable composition containing ground non-expanded pearlite present in an amount of from about 1% to about 75% of the weight of the cementing components in the settable composition, cement kiln dust, pumicite, and functional additives. The invention is developed in the dependent claims of the invention formula.EFFECT: increased efficiency of cementing.20 cl, 6 tbl, 6 ex
Изобретение относится к операциям цементирования. Вариант осуществления настоящего изобретения включает способную к схватыванию композицию, содержащую размолотый невспученный перлит, пумицит, цементную печную пыль и воду. Другой вариант осуществления настоящего изобретения включает способную к схватыванию композицию, содержащую размолотый невспученный перлит, присутствующий в количестве от примерно 1% до примерно 75% от массы цементирующих компонентов в способной к схватыванию композиции, причем размолотый невспученный перлит имеет средний размер частиц от примерно 1 мкм до примерно 100 мкм, цементную печную пыль, размолотую смесь цемента и пумицита и воду. Еще один вариант осуществления настоящего изобретения включает способную к схватыванию композицию, содержащую размолотый невспученный перлит, присутствующий в количестве от примерно 1% до примерно 75% от массы цементирующих компонентов в способной к схватыванию композиции, цементную печную пыль, пумицит и функциональные добавки. Изобретение развито в зависимых пунктах формулы изобретения. Технический результат - повышение эффективности цементирования. 3 н. и 17 з.п. ф-лы, 6 табл., 6 пр.
SETTABLE COMPOSITIONS CONTAINING NON-EXPANDED PEARLITE (VERSIONS)
СПОСОБНЫЕ К СХВАТЫВАНИЮ КОМПОЗИЦИИ, СОДЕРЖАЩИЕ НЕВСПУЧЕННЫЙ ПЕРЛИТ (ВАРИАНТЫ)
BRENNAJS CHED D (Autor:in) / KARCHER DZHEFFRI D (Autor:in) / RODDI KREJG UEJN (Autor:in)
06.12.2017
Patent
Elektronische Ressource
Russisch