Expanded lightweight aggregate made from glass or pumice
An expanded lightweight aggregate has compositional ranges (Wt. % Range) of about: (a) 40 to 60% ground glass or pumice, 40 to 60% water, 3 to 15% sodium silicate, and 0.1 to 5% NaNO3 for the slurry; and (b) 50 to 85% ground glass or pumice, and 15 to 50% slurry for the granulator.
Expanded lightweight aggregate made from glass or pumice
An expanded lightweight aggregate has compositional ranges (Wt. % Range) of about: (a) 40 to 60% ground glass or pumice, 40 to 60% water, 3 to 15% sodium silicate, and 0.1 to 5% NaNO3 for the slurry; and (b) 50 to 85% ground glass or pumice, and 15 to 50% slurry for the granulator.
Expanded lightweight aggregate made from glass or pumice
DANIELS EVAN R (Autor:in) / ANDERSEN PER JUST (Autor:in)
25.10.2016
Patent
Elektronische Ressource
Englisch
IPC:
C04B
Kalk
,
LIME
EXPANDED LIGHTWEIGHT AGGREGATE MADE FROM GLASS OR PUMICE
Europäisches Patentamt | 2017
|Expanded lightweight aggregate made from glass or pumice
Europäisches Patentamt | 2017
|Expanded Lightweight Aggregate Made From Glass or Pumice
Europäisches Patentamt | 2016
|Expanded Lightweight Aggregate Made From Glass or Pumice
Europäisches Patentamt | 2017
|Engineering Index Backfile | 1951
|