PIEZOELECTRIC CERAMIC ELECTRONIC COMPONENT, AND METHOD FOR MANUFACTURING PIEZOELECTRIC CERAMIC ELECTRONIC COMPONENT
In a piezoelectric ceramic electronic component, internal electrodes 3 are embedded in a piezoelectric ceramic element assembly 1. The piezoelectric ceramic element assembly 1 contains Zr, a lead-free perovskite compound including at least Li and Nb, and a composite oxide including a bivalent metallic element. The molar content of Li and the bivalent metallic element, and the combined molar content thereof are 0.025-0.080 part by mole, 0.045-0.086 part by mole, and 0.076-0.166 part by mole, respectively, with respect to 1 part by mole of Nb. The internal electrodes 3 contain Ni. The piezoelectric ceramic element assembly 1 is obtained by performing calcining synthesis of the perovskite compound, then adding a metallic element compound and a Zr compound thereto and performing calcining synthesis again, and then firing the product. By adjusting the blending ratio of the lead-free piezoelectric ceramic composition, a lead-free piezoelectric ceramic electronic component and a method for manufacturing the same are obtained whereby piezoelectric characteristics can be further enhanced relative to the prior art even when firing is performed together with Ni.
Dans un composant électronique céramique piézoélectrique, des électrodes internes 3 sont incorporées dans un ensemble 1 d'éléments céramiques piézoélectriques. L'ensemble 1 d'éléments céramiques piézoélectriques contient Zr, un composé pérovskite sans plomb comprenant au moins Li et Nb, et un oxyde composite comprenant un élément métallique bivalent. La teneur en moles de Li et de l'élément métallique bivalent, et leur teneur en moles combinée, sont respectivement de 0,025 à 0,080 partie en moles, de 0,045 à 0,086 partie en moles, et de 0,076 à 0,166 partie en moles, pour 1 partie en moles de Nb. Les électrodes internes 3 contiennent Ni. L'ensemble 1 d'éléments céramiques piézoélectriques est obtenu par mise en œuvre d'une synthèse par calcination du composé pérovskite, puis addition d'un composé d'un élément métallique et d'un composé de Zr, et mise en œuvre de nouveau d'une synthèse par calcination, puis cuisson du produit. Par ajustement du rapport de mélange de la composition céramique piézoélectrique sans plomb, on obtient un composant électronique céramique piézoélectrique sans plomb et un procédé de fabrication de ce dernier, par lesquels il est possible de renforcer encore plus les caractéristiques piézoélectriques par rapport à la technique antérieure, même si la cuisson est mise en œuvre en même temps qu'avec Ni.
圧電セラミック電子部品は、圧電セラミック素体1に内部電極3が埋設されている。圧電セラミック素体1は、少なくともLi及びNbを含む非鉛系のペロブスカイト化合物、Zr、及び2価の金属元素を含む複合酸化物を含有している。Li、2価の金属元素、及びこれらの総計の含有モル量は、それぞれNb1モル部に対し0.025~0.080モル部、0.045~0.086モル部、0.076~0.166モル部である。内部電極3はNiを含有している。ペロブスカイト化合物を仮焼合成した後、これに金属元素化合物及びZr化合物を添加して再度仮焼合成し、その後焼成して圧電セラミック素体1を得る。非鉛系圧電磁器組成物の配合比率を調整することで、Niと共焼成しても従来に比べ更なる圧電特性の向上が可能な非鉛系の圧電セラミック電子部品とその製造方法を実現する。
PIEZOELECTRIC CERAMIC ELECTRONIC COMPONENT, AND METHOD FOR MANUFACTURING PIEZOELECTRIC CERAMIC ELECTRONIC COMPONENT
In a piezoelectric ceramic electronic component, internal electrodes 3 are embedded in a piezoelectric ceramic element assembly 1. The piezoelectric ceramic element assembly 1 contains Zr, a lead-free perovskite compound including at least Li and Nb, and a composite oxide including a bivalent metallic element. The molar content of Li and the bivalent metallic element, and the combined molar content thereof are 0.025-0.080 part by mole, 0.045-0.086 part by mole, and 0.076-0.166 part by mole, respectively, with respect to 1 part by mole of Nb. The internal electrodes 3 contain Ni. The piezoelectric ceramic element assembly 1 is obtained by performing calcining synthesis of the perovskite compound, then adding a metallic element compound and a Zr compound thereto and performing calcining synthesis again, and then firing the product. By adjusting the blending ratio of the lead-free piezoelectric ceramic composition, a lead-free piezoelectric ceramic electronic component and a method for manufacturing the same are obtained whereby piezoelectric characteristics can be further enhanced relative to the prior art even when firing is performed together with Ni.
Dans un composant électronique céramique piézoélectrique, des électrodes internes 3 sont incorporées dans un ensemble 1 d'éléments céramiques piézoélectriques. L'ensemble 1 d'éléments céramiques piézoélectriques contient Zr, un composé pérovskite sans plomb comprenant au moins Li et Nb, et un oxyde composite comprenant un élément métallique bivalent. La teneur en moles de Li et de l'élément métallique bivalent, et leur teneur en moles combinée, sont respectivement de 0,025 à 0,080 partie en moles, de 0,045 à 0,086 partie en moles, et de 0,076 à 0,166 partie en moles, pour 1 partie en moles de Nb. Les électrodes internes 3 contiennent Ni. L'ensemble 1 d'éléments céramiques piézoélectriques est obtenu par mise en œuvre d'une synthèse par calcination du composé pérovskite, puis addition d'un composé d'un élément métallique et d'un composé de Zr, et mise en œuvre de nouveau d'une synthèse par calcination, puis cuisson du produit. Par ajustement du rapport de mélange de la composition céramique piézoélectrique sans plomb, on obtient un composant électronique céramique piézoélectrique sans plomb et un procédé de fabrication de ce dernier, par lesquels il est possible de renforcer encore plus les caractéristiques piézoélectriques par rapport à la technique antérieure, même si la cuisson est mise en œuvre en même temps qu'avec Ni.
圧電セラミック電子部品は、圧電セラミック素体1に内部電極3が埋設されている。圧電セラミック素体1は、少なくともLi及びNbを含む非鉛系のペロブスカイト化合物、Zr、及び2価の金属元素を含む複合酸化物を含有している。Li、2価の金属元素、及びこれらの総計の含有モル量は、それぞれNb1モル部に対し0.025~0.080モル部、0.045~0.086モル部、0.076~0.166モル部である。内部電極3はNiを含有している。ペロブスカイト化合物を仮焼合成した後、これに金属元素化合物及びZr化合物を添加して再度仮焼合成し、その後焼成して圧電セラミック素体1を得る。非鉛系圧電磁器組成物の配合比率を調整することで、Niと共焼成しても従来に比べ更なる圧電特性の向上が可能な非鉛系の圧電セラミック電子部品とその製造方法を実現する。
PIEZOELECTRIC CERAMIC ELECTRONIC COMPONENT, AND METHOD FOR MANUFACTURING PIEZOELECTRIC CERAMIC ELECTRONIC COMPONENT
COMPOSANT ÉLECTRONIQUE CÉRAMIQUE PIÉZOÉLECTRIQUE ET PROCÉDÉ DE FABRICATION D'UN COMPOSANT ÉLECTRONIQUE CÉRAMIQUE PIÉZOÉLECTRIQUE
圧電セラミック電子部品、及び圧電セラミック電子部品の製造方法
ISHII HIDEKI (Autor:in) / HAYASHI HIROYUKI (Autor:in) / KAWADA SHINICHIRO (Autor:in) / OGAWA HIROZUMI (Autor:in)
12.01.2017
Patent
Elektronische Ressource
Japanisch
Europäisches Patentamt | 2015
|Europäisches Patentamt | 2023
|Europäisches Patentamt | 2018
|Europäisches Patentamt | 2021
|Europäisches Patentamt | 2018
|