METHOD FOR PRODUCING CONJUGATE, AND CONJUGATE
The method for producing a conjugate has (a) a step for preparing an aluminum member, a ceramic member, and an alloy member including silicon and aluminum, the thermal expansion coefficient of the alloy member being smaller than that of the aluminum member and larger than that of the ceramic member, (b) a step for installing a first bonding material on a bonding surface of the aluminum member and/or a first surface of the alloy member as well as installing a second bonding material on a bonding surface of the ceramic member and/or a second surface of the alloy member, (c) a step for laminating the aluminum member, alloy member, and ceramic member in that order and constructing an assembly, and (d) a step for heating the assembly at a temperature of 400-800°C in an inert gas atmosphere or a vacuum atmosphere.
La présente invention concerne un procédé de production d'un conjugué qui comprend (a) une étape de préparation d'un élément en aluminium, d'un élément en céramique, et d'un élément en alliage comprenant du silicium et de l'aluminium, le coefficient de dilatation thermique de l'élément en alliage étant inférieur à celui de l'élément en aluminium et supérieur à celui de l'élément en céramique, (b) une étape d'installation d'un premier matériau de liaison sur une surface de liaison de l'élément en aluminium et/ou une première surface de l'élément en alliage ainsi que l'installation d'un second matériau de liaison sur une surface de liaison de l'élément en céramique et/ou une seconde surface de l'élément en alliage, (c) une étape de stratification de l'élément en aluminium, de l'élément en alliage et de l'élément en céramique dans cet ordre et de construction d'un ensemble, et (d) une étape de chauffage de l'ensemble à une température de 400 à 800 °C dans une atmosphère de gaz inerte ou une atmosphère sous vide.
本接合体の製造方法は、(a)アルミニウム部材、セラミックス部材、ならびにケイ素およびアルミニウムを含む合金部材を準備するステップであって、前記合金部材の熱膨張係数は、前記アルミニウム部材よりも小さく、前記セラミックス部材よりも大きい、ステップと、(b)アルミニウム部材の被接合面および合金部材の第1の表面の少なくとも一方に、第1の接合材を設置するとともに、セラミックス部材の被接合面および合金部材の第2の表面の少なくとも一方に、第2の接合材を設置する、ステップと、(c)アルミニウム部材、合金部材、およびセラミックス部材を、この順に積層し、組立体を構成するステップと、(d)前記組立体を、不活性ガス雰囲気下または真空雰囲気下、400℃~800℃の温度で加熱するステップと、を有する。
METHOD FOR PRODUCING CONJUGATE, AND CONJUGATE
The method for producing a conjugate has (a) a step for preparing an aluminum member, a ceramic member, and an alloy member including silicon and aluminum, the thermal expansion coefficient of the alloy member being smaller than that of the aluminum member and larger than that of the ceramic member, (b) a step for installing a first bonding material on a bonding surface of the aluminum member and/or a first surface of the alloy member as well as installing a second bonding material on a bonding surface of the ceramic member and/or a second surface of the alloy member, (c) a step for laminating the aluminum member, alloy member, and ceramic member in that order and constructing an assembly, and (d) a step for heating the assembly at a temperature of 400-800°C in an inert gas atmosphere or a vacuum atmosphere.
La présente invention concerne un procédé de production d'un conjugué qui comprend (a) une étape de préparation d'un élément en aluminium, d'un élément en céramique, et d'un élément en alliage comprenant du silicium et de l'aluminium, le coefficient de dilatation thermique de l'élément en alliage étant inférieur à celui de l'élément en aluminium et supérieur à celui de l'élément en céramique, (b) une étape d'installation d'un premier matériau de liaison sur une surface de liaison de l'élément en aluminium et/ou une première surface de l'élément en alliage ainsi que l'installation d'un second matériau de liaison sur une surface de liaison de l'élément en céramique et/ou une seconde surface de l'élément en alliage, (c) une étape de stratification de l'élément en aluminium, de l'élément en alliage et de l'élément en céramique dans cet ordre et de construction d'un ensemble, et (d) une étape de chauffage de l'ensemble à une température de 400 à 800 °C dans une atmosphère de gaz inerte ou une atmosphère sous vide.
本接合体の製造方法は、(a)アルミニウム部材、セラミックス部材、ならびにケイ素およびアルミニウムを含む合金部材を準備するステップであって、前記合金部材の熱膨張係数は、前記アルミニウム部材よりも小さく、前記セラミックス部材よりも大きい、ステップと、(b)アルミニウム部材の被接合面および合金部材の第1の表面の少なくとも一方に、第1の接合材を設置するとともに、セラミックス部材の被接合面および合金部材の第2の表面の少なくとも一方に、第2の接合材を設置する、ステップと、(c)アルミニウム部材、合金部材、およびセラミックス部材を、この順に積層し、組立体を構成するステップと、(d)前記組立体を、不活性ガス雰囲気下または真空雰囲気下、400℃~800℃の温度で加熱するステップと、を有する。
METHOD FOR PRODUCING CONJUGATE, AND CONJUGATE
PROCÉDÉ DE PRODUCTION D'UN CONJUGUÉ, ET CONJUGUÉ
接合体の製造方法および接合体