CUBIC BORON NITRIDE SINTERED BODY AND METHOD FOR MANUFACTURING SAME
A cubic boron nitride sintered body according to the present invention is provided with 40-85 vol%, inclusive, of cubic boron nitride particles and a bonded phase. The bonded phase includes one or more first compounds comprising at least one element selected from the group comprising titanium, zirconium, hafnium, vanadium, niobium, tantalum, chrome, molybdenum, and tungsten and at least one element selected from the group comprising nitrogen, carbon, boron, and oxygen, and at least one selected from the group comprising solid solutions derived from the first compound, or, at least one selected from the group consisting of one or more first compounds and a solid solution derived from the first compound, and an aluminum compound. The cubic boron nitride particles, in terms of the numbers thereof, include 50% or more of cubic boron nitride particles having an equivalent circle diameter greater than 0.5 µm and 50% or less of cubic boron nitride particles having an equivalent circle diameter greater than 2 µm. If the mass of the cubic boron nitride particles is 100 mass%, the total content of lithium, magnesium, calcium, strontium, beryllium, and barium in the cubic boron nitride particles is less than 0.001 mass%.
Le corps fritté de nitrure de bore cubique de l'invention est équipé de 40% en volume ou plus à 85% en volume ou moins de particules de nitrure de bore cubique, et d'une phase de liaison. Ladite phase de liaison contient soit d'une part au moins un élément chimique choisi dans un groupe constitué d'un titane, d'un zirconium, d'un hafnium, d'un vanadium, d'un niobium, d'un tantale, d'un chrome, d'un molybdène et d'un tungstène, et d'autre part au moins un élément choisi dans un groupe constitué d'au moins une sorte de premier composé constitué d'au moins un élément chimique choisi dans un groupe constitué d'un azote, d'un carbone, d'un bore et d'un oxygène, et d'une solution solide dérivée dudit premier composé, soit d'une part au moins un élément choisi dans un groupe constitué au moins de ladite sorte de premier composé, et d'une solution solide dérivée dudit premier composé, et d'autre part un composé aluminium. Lesdites particules de nitrure de bore cubique contiennent : 50% ou plus en termes de nombres de particules de nitrure de bore cubique de diamètre de cercle équivalent supérieur à 0,5μm ; et 50% ou moins en termes de nombres de particules de nitrure de bore cubique de diamètre de cercle équivalent supérieur à 2μm. Dans le cas où la masse desdites particules de nitrure de bore cubique représente 100% en masse, la teneur totale en lithium, magnésium, calcium, strontium, béryllium et baryum dans lesdites particules de nitrure de bore cubique, est inférieure à 0,001% en masse.
立方晶窒化硼素焼結体は、40体積%以上85体積%以下の立方晶窒化硼素粒子と、結合相と、を備える立方晶窒化硼素焼結体であって、前記結合相は、チタン、ジルコニウム、ハフニウム、バナジウム、ニオブ、タンタル、クロム、モリブデン及びタングステンからなる群より選ばれる少なくとも1種の元素と、窒素、炭素、硼素及び酸素からなる群より選ばれる少なくとも1種の元素とからなる1種以上の第1化合物、並びに、前記第1化合物由来の固溶体からなる群より選ばれる少なくとも1種、又は、1種以上の前記第1化合物及び前記第1化合物由来の固溶体からなる群より選ばれる少なくとも1種と、アルミニウム化合物と、を含み、前記立方晶窒化硼素粒子は、円相当径が0.5μm超の立方晶窒化硼素粒子を数基準で50%以上、かつ、円相当径が2μm超の立方晶窒化硼素粒子を数基準で50%以下含み、前記立方晶窒化硼素粒子の質量を100質量%とした場合、前記立方晶窒化硼素粒子中のリチウム、マグネシウム、カルシウム、ストロンチウム、ベリリウム及びバリウムの合計含有量は0.001質量%未満である。
CUBIC BORON NITRIDE SINTERED BODY AND METHOD FOR MANUFACTURING SAME
A cubic boron nitride sintered body according to the present invention is provided with 40-85 vol%, inclusive, of cubic boron nitride particles and a bonded phase. The bonded phase includes one or more first compounds comprising at least one element selected from the group comprising titanium, zirconium, hafnium, vanadium, niobium, tantalum, chrome, molybdenum, and tungsten and at least one element selected from the group comprising nitrogen, carbon, boron, and oxygen, and at least one selected from the group comprising solid solutions derived from the first compound, or, at least one selected from the group consisting of one or more first compounds and a solid solution derived from the first compound, and an aluminum compound. The cubic boron nitride particles, in terms of the numbers thereof, include 50% or more of cubic boron nitride particles having an equivalent circle diameter greater than 0.5 µm and 50% or less of cubic boron nitride particles having an equivalent circle diameter greater than 2 µm. If the mass of the cubic boron nitride particles is 100 mass%, the total content of lithium, magnesium, calcium, strontium, beryllium, and barium in the cubic boron nitride particles is less than 0.001 mass%.
Le corps fritté de nitrure de bore cubique de l'invention est équipé de 40% en volume ou plus à 85% en volume ou moins de particules de nitrure de bore cubique, et d'une phase de liaison. Ladite phase de liaison contient soit d'une part au moins un élément chimique choisi dans un groupe constitué d'un titane, d'un zirconium, d'un hafnium, d'un vanadium, d'un niobium, d'un tantale, d'un chrome, d'un molybdène et d'un tungstène, et d'autre part au moins un élément choisi dans un groupe constitué d'au moins une sorte de premier composé constitué d'au moins un élément chimique choisi dans un groupe constitué d'un azote, d'un carbone, d'un bore et d'un oxygène, et d'une solution solide dérivée dudit premier composé, soit d'une part au moins un élément choisi dans un groupe constitué au moins de ladite sorte de premier composé, et d'une solution solide dérivée dudit premier composé, et d'autre part un composé aluminium. Lesdites particules de nitrure de bore cubique contiennent : 50% ou plus en termes de nombres de particules de nitrure de bore cubique de diamètre de cercle équivalent supérieur à 0,5μm ; et 50% ou moins en termes de nombres de particules de nitrure de bore cubique de diamètre de cercle équivalent supérieur à 2μm. Dans le cas où la masse desdites particules de nitrure de bore cubique représente 100% en masse, la teneur totale en lithium, magnésium, calcium, strontium, béryllium et baryum dans lesdites particules de nitrure de bore cubique, est inférieure à 0,001% en masse.
立方晶窒化硼素焼結体は、40体積%以上85体積%以下の立方晶窒化硼素粒子と、結合相と、を備える立方晶窒化硼素焼結体であって、前記結合相は、チタン、ジルコニウム、ハフニウム、バナジウム、ニオブ、タンタル、クロム、モリブデン及びタングステンからなる群より選ばれる少なくとも1種の元素と、窒素、炭素、硼素及び酸素からなる群より選ばれる少なくとも1種の元素とからなる1種以上の第1化合物、並びに、前記第1化合物由来の固溶体からなる群より選ばれる少なくとも1種、又は、1種以上の前記第1化合物及び前記第1化合物由来の固溶体からなる群より選ばれる少なくとも1種と、アルミニウム化合物と、を含み、前記立方晶窒化硼素粒子は、円相当径が0.5μm超の立方晶窒化硼素粒子を数基準で50%以上、かつ、円相当径が2μm超の立方晶窒化硼素粒子を数基準で50%以下含み、前記立方晶窒化硼素粒子の質量を100質量%とした場合、前記立方晶窒化硼素粒子中のリチウム、マグネシウム、カルシウム、ストロンチウム、ベリリウム及びバリウムの合計含有量は0.001質量%未満である。
CUBIC BORON NITRIDE SINTERED BODY AND METHOD FOR MANUFACTURING SAME
CORPS FRITTÉ DE NITRURE DE BORE CUBIQUE, ET PROCÉDÉ DE FABRICATION DE CELUI-CI
立方晶窒化硼素焼結体及びその製造方法
ABE MACHIKO (Autor:in) / KUKINO SATORU (Autor:in) / MATSUKAWA MICHIKO (Autor:in) / HIGASHI TAISUKE (Autor:in)
24.06.2021
Patent
Elektronische Ressource
Japanisch
IPC:
C04B
Kalk
,
LIME
Europäisches Patentamt | 2022
|METHOD FOR MANUFACTURING CUBIC BORON NITRIDE SINTERED BODY AND CUBIC BORON NITRIDE SINTERED BODY
Europäisches Patentamt | 2017
METHOD FOR MANUFACTURING CUBIC BORON NITRIDE SINTERED BODY, AND CUBIC BORON NITRIDE SINTERED BODY
Europäisches Patentamt | 2016
|METHOD FOR MANUFACTURING CUBIC BORON NITRIDE SINTERED BODY, AND CUBIC BORON NITRIDE SINTERED BODY
Europäisches Patentamt | 2020
|Method for manufacturing cubic boron nitride sintered body, and cubic boron nitride sintered body
Europäisches Patentamt | 2016
|