GELLING AGENT FOR CURING HEAVY METAL IONS IN TAILINGS AND USE METHOD THEREOF
Disclosed are a gelling agent for curing heavy metal ions in tailings and a use method thereof. The gelling agent comprises the following raw materials in mass percent: 0.25-0.7% of a chelating trapping agent, 0.15-0.3% of a chelating accelerant, 0.2-0.6% of a complexing early strength agent, 1-7% of lime, 0-10% of cement, 8-20% of gypsum, 0-20% of steel slag micro powder, and 50-82% of mineral slag micro powder. The chelating trapping agent, the chelating accelerant and the complexing early strength agent are mixed well first, and then mixed with other components uniformly. The gelling agent prepared in the present invention can be used for not only cementing total tailings by means of hydration to achieve filling mining, but also synergistically curing heavy metal ions in the tailings by means of leaching, chelating, wrapping, chemical adsorption, chemical passivation, ion substitution and the like to maintain the curing stability for a long time. The gelling agent is particularly suitable for cemented filling of total tailings having high heavy metal ion content, and significantly reduces the environmental risk of high content of heavy metal ions in the filling body after tailings filling.
L'invention concerne un agent gélifiant destiné à durcir des ions de métaux lourds dans des résidus, ainsi que son procédé d'utilisation. L'agent gélifiant selon l'invention comprend les matières premières suivantes, en pourcentage en masse : de 0,25 à 0,7 % d'agent de piégeage chélateur, de 0,15 à 0,3 % d'accélérateur de chélation, de 0,2 à 0,6 % d'agent de résistance initiale complexant, de 1 à 7 % de chaux, de 0 à 10 % de ciment, de 8 à 20 % de gypse, de 0 à 20 % de micro-poudre de laitier d'acier, et de 50 à 82 % de micro-poudre de laitier minéral. L'agent de piégeage chélateur, l'accélérateur de chélation et l'agent de résistance initiale complexant sont d'abord bien mélangés, puis ils sont mélangés avec d'autres composants, de façon uniforme. L'agent gélifiant préparé selon la présente invention peut être utilisé non seulement pour cimenter des résidus totaux par hydratation afin d'obtenir un remplissage minier, mais également pour durcir de façon synergique des ions de métaux lourds dans les résidus par lixiviation, chélation, enrobage, adsorption chimique, passivation chimique, substitution d'ions et analogues, afin de maintenir la stabilité de durcissement pendant une longue durée. L'agent gélifiant selon l'invention est particulièrement approprié pour le remplissage cimenté de résidus totaux présentant une teneur élevée en ions de métaux lourds, et réduit considérablement le risque environnemental lié à une teneur élevée en ions de métaux lourds dans le corps de remplissage, après remplissage de résidus.
本发明公开了一种用于固化尾矿中重金属离子的胶凝剂及其使用方法,原料中各组份的质量百分含量为:螯合捕捉剂0.25~0.7%,螯合促进剂0.15~0.3%,络合早强剂0.2~0.6%,石灰1~7%,水泥0~10%,石膏8~20%,钢渣微粉0~20%,矿渣微粉50~82%。先将螯合捕捉剂螯合促进剂络合早强剂混合均匀,再与其它组份混合均匀。本发明制备的胶凝剂不仅通过水化反应胶结全尾矿,实现充填开采,还通过浸出、螯合、包裹、化学吸附、化学钝化和离子替代等多种作用协同固化尾矿中重金属离子,长期保持固化的稳定性,特别适用于重金属离子含量高的全尾矿胶结充填,显著降低尾矿充填后充填体重金属离子含量高的环境风险。
GELLING AGENT FOR CURING HEAVY METAL IONS IN TAILINGS AND USE METHOD THEREOF
Disclosed are a gelling agent for curing heavy metal ions in tailings and a use method thereof. The gelling agent comprises the following raw materials in mass percent: 0.25-0.7% of a chelating trapping agent, 0.15-0.3% of a chelating accelerant, 0.2-0.6% of a complexing early strength agent, 1-7% of lime, 0-10% of cement, 8-20% of gypsum, 0-20% of steel slag micro powder, and 50-82% of mineral slag micro powder. The chelating trapping agent, the chelating accelerant and the complexing early strength agent are mixed well first, and then mixed with other components uniformly. The gelling agent prepared in the present invention can be used for not only cementing total tailings by means of hydration to achieve filling mining, but also synergistically curing heavy metal ions in the tailings by means of leaching, chelating, wrapping, chemical adsorption, chemical passivation, ion substitution and the like to maintain the curing stability for a long time. The gelling agent is particularly suitable for cemented filling of total tailings having high heavy metal ion content, and significantly reduces the environmental risk of high content of heavy metal ions in the filling body after tailings filling.
L'invention concerne un agent gélifiant destiné à durcir des ions de métaux lourds dans des résidus, ainsi que son procédé d'utilisation. L'agent gélifiant selon l'invention comprend les matières premières suivantes, en pourcentage en masse : de 0,25 à 0,7 % d'agent de piégeage chélateur, de 0,15 à 0,3 % d'accélérateur de chélation, de 0,2 à 0,6 % d'agent de résistance initiale complexant, de 1 à 7 % de chaux, de 0 à 10 % de ciment, de 8 à 20 % de gypse, de 0 à 20 % de micro-poudre de laitier d'acier, et de 50 à 82 % de micro-poudre de laitier minéral. L'agent de piégeage chélateur, l'accélérateur de chélation et l'agent de résistance initiale complexant sont d'abord bien mélangés, puis ils sont mélangés avec d'autres composants, de façon uniforme. L'agent gélifiant préparé selon la présente invention peut être utilisé non seulement pour cimenter des résidus totaux par hydratation afin d'obtenir un remplissage minier, mais également pour durcir de façon synergique des ions de métaux lourds dans les résidus par lixiviation, chélation, enrobage, adsorption chimique, passivation chimique, substitution d'ions et analogues, afin de maintenir la stabilité de durcissement pendant une longue durée. L'agent gélifiant selon l'invention est particulièrement approprié pour le remplissage cimenté de résidus totaux présentant une teneur élevée en ions de métaux lourds, et réduit considérablement le risque environnemental lié à une teneur élevée en ions de métaux lourds dans le corps de remplissage, après remplissage de résidus.
本发明公开了一种用于固化尾矿中重金属离子的胶凝剂及其使用方法,原料中各组份的质量百分含量为:螯合捕捉剂0.25~0.7%,螯合促进剂0.15~0.3%,络合早强剂0.2~0.6%,石灰1~7%,水泥0~10%,石膏8~20%,钢渣微粉0~20%,矿渣微粉50~82%。先将螯合捕捉剂螯合促进剂络合早强剂混合均匀,再与其它组份混合均匀。本发明制备的胶凝剂不仅通过水化反应胶结全尾矿,实现充填开采,还通过浸出、螯合、包裹、化学吸附、化学钝化和离子替代等多种作用协同固化尾矿中重金属离子,长期保持固化的稳定性,特别适用于重金属离子含量高的全尾矿胶结充填,显著降低尾矿充填后充填体重金属离子含量高的环境风险。
GELLING AGENT FOR CURING HEAVY METAL IONS IN TAILINGS AND USE METHOD THEREOF
AGENT GÉLIFIANT DESTINÉ À DURCIR DES IONS DE MÉTAUX LOURDS DANS DES RÉSIDUS ET PROCÉDÉ D'UTILISATION ASSOCIÉ
一种用于固化尾矿中重金属离子的胶凝剂及其使用方法
YANG XIAOJUN (Autor:in) / XU XIUPING (Autor:in) / HUA SHAOGUANG (Autor:in) / LIU LONG (Autor:in) / YU XIANKUN (Autor:in)
04.08.2022
Patent
Elektronische Ressource
Chinesisch
IPC:
C04B
Kalk
,
LIME
Gelling agent for curing heavy metal ions in tailings and use method thereof
Europäisches Patentamt | 2021
|Europäisches Patentamt | 2024
|Aluminum base gelling and curing agent, preparation method and application thereof
Europäisches Patentamt | 2015
|Europäisches Patentamt | 2024
|Special curing agent for curing steel tailings and application method
Europäisches Patentamt | 2020
|