HEAT STORAGE GRAPHITE HAVING LOW DEGREE OF ORIENTATION, COMPOSITION FOR PREPARING HEAT STORAGE GRAPHITE HAVING LOW DEGREE OF ORIENTATION, AND METHOD THEREFOR
Provided are heat storage graphite having a low degree of orientation, a composition for preparing heat storage graphite having a low degree of orientation, and a method for preparing heat storage graphite having a low degree of orientation. The heat storage graphite comprises, in terms of the total mass of the heat storage graphite, 65-85wt% of dispersed-phase graphite and 15-35wt% of continuous-phase graphite, wherein the dispersed-phase graphite is spherical graphite, and the sphericity of the spherical graphite is 0.5-1; the ratio of the vertical thermal conductivity/plane-oriented thermal conductivity of the heat storage graphite is 0.4 - 0.8; and the plane-oriented thermal conductivity of the heat storage graphite is 50-150 W/mK. The heat storage graphite has the advantages of a low degree of orientation and high plane-oriented thermal conductivity.
L'invention concerne un graphite de stockage de chaleur ayant un faible degré d'orientation, une composition pour la préparation de graphite de stockage de chaleur ayant un faible degré d'orientation, et un procédé de préparation de graphite de stockage de chaleur ayant un faible degré d'orientation. Le graphite de stockage de chaleur comprend, en termes de masse totale du graphite de stockage de chaleur, de 65 à 85 % en poids de graphite en phase dispersée et de 15 à 35 % en poids de graphite en phase continue, le graphite en phase dispersée étant du graphite sphérique, et la sphéricité du graphite sphérique étant de 0,5 à 1 ; le rapport de la conductivité thermique verticale/conductivité thermique orientée dans le plan du graphite de stockage de chaleur étant de 0,4 à 0,8 ; et la conductivité thermique orientée dans le plan du graphite de stockage de chaleur étant de 50 à 150 W/mK. Le graphite de stockage de chaleur présente les avantages d'un faible degré d'orientation et d'une conductivité thermique orientée dans le plan élevée.
提供了一种低取向度储热石墨、制备低取向度储热石墨的组合物及低取向度储热石墨的制备方法,以储热石墨的总质量计,储热石墨包括65-85wt%的分散相石墨和15-35wt%的连续相石墨;其中,分散相石墨为球形石墨,球形石墨的球度为0.5-1;储热石墨的垂直热导率/面向热导率的比值为0.4-0.8,储热石墨的面向热导率为50-150W/mK。储热石墨具有取向度低且面向热导率高的优点。
HEAT STORAGE GRAPHITE HAVING LOW DEGREE OF ORIENTATION, COMPOSITION FOR PREPARING HEAT STORAGE GRAPHITE HAVING LOW DEGREE OF ORIENTATION, AND METHOD THEREFOR
Provided are heat storage graphite having a low degree of orientation, a composition for preparing heat storage graphite having a low degree of orientation, and a method for preparing heat storage graphite having a low degree of orientation. The heat storage graphite comprises, in terms of the total mass of the heat storage graphite, 65-85wt% of dispersed-phase graphite and 15-35wt% of continuous-phase graphite, wherein the dispersed-phase graphite is spherical graphite, and the sphericity of the spherical graphite is 0.5-1; the ratio of the vertical thermal conductivity/plane-oriented thermal conductivity of the heat storage graphite is 0.4 - 0.8; and the plane-oriented thermal conductivity of the heat storage graphite is 50-150 W/mK. The heat storage graphite has the advantages of a low degree of orientation and high plane-oriented thermal conductivity.
L'invention concerne un graphite de stockage de chaleur ayant un faible degré d'orientation, une composition pour la préparation de graphite de stockage de chaleur ayant un faible degré d'orientation, et un procédé de préparation de graphite de stockage de chaleur ayant un faible degré d'orientation. Le graphite de stockage de chaleur comprend, en termes de masse totale du graphite de stockage de chaleur, de 65 à 85 % en poids de graphite en phase dispersée et de 15 à 35 % en poids de graphite en phase continue, le graphite en phase dispersée étant du graphite sphérique, et la sphéricité du graphite sphérique étant de 0,5 à 1 ; le rapport de la conductivité thermique verticale/conductivité thermique orientée dans le plan du graphite de stockage de chaleur étant de 0,4 à 0,8 ; et la conductivité thermique orientée dans le plan du graphite de stockage de chaleur étant de 50 à 150 W/mK. Le graphite de stockage de chaleur présente les avantages d'un faible degré d'orientation et d'une conductivité thermique orientée dans le plan élevée.
提供了一种低取向度储热石墨、制备低取向度储热石墨的组合物及低取向度储热石墨的制备方法,以储热石墨的总质量计,储热石墨包括65-85wt%的分散相石墨和15-35wt%的连续相石墨;其中,分散相石墨为球形石墨,球形石墨的球度为0.5-1;储热石墨的垂直热导率/面向热导率的比值为0.4-0.8,储热石墨的面向热导率为50-150W/mK。储热石墨具有取向度低且面向热导率高的优点。
HEAT STORAGE GRAPHITE HAVING LOW DEGREE OF ORIENTATION, COMPOSITION FOR PREPARING HEAT STORAGE GRAPHITE HAVING LOW DEGREE OF ORIENTATION, AND METHOD THEREFOR
GRAPHITE DE STOCKAGE DE CHALEUR AYANT UN FAIBLE DEGRÉ D'ORIENTATION, COMPOSITION POUR LA PRÉPARATION DE GRAPHITE DE STOCKAGE DE CHALEUR AYANT UN FAIBLE DEGRÉ D'ORIENTATION, ET PROCÉDÉ ASSOCIÉ
低取向度储热石墨、制备低取向度储热石墨的组合物及其制备方法
DUAN CHUNTING (Autor:in) / WEI CHANG (Autor:in) / LIANG WENBIN (Autor:in) / LIU JUNQING (Autor:in) / ZHENG DONGFANG (Autor:in) / GAO GUANGHUI (Autor:in) / SHENG YING (Autor:in) / WEN CHENGYU (Autor:in)
06.10.2022
Patent
Elektronische Ressource
Chinesisch
Europäisches Patentamt | 2024
|Europäisches Patentamt | 2024
|Europäisches Patentamt | 2024
|Europäisches Patentamt | 2020
|Europäisches Patentamt | 2020