A platform for research: civil engineering, architecture and urbanism
Laser nitriding of pure titanium with Ni, Cr for improved wear performance
Laser nitriding of pure titanium with Ni, Cr for improved wear performance
Laser nitriding of pure titanium with Ni, Cr for improved wear performance
Fu, Y. (author) / Batchelor, A. W. (author)
WEAR -LAUSANNE- ; 214 ; 83-90
1998-01-01
8 pages
Article (Journal)
English
DDC:
620.11292
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Crack-Free Wear Resistance Coatings Produced on Pure Titanium and Ti-6Al-4V by Laser Nitriding
British Library Online Contents | 2005
|Low Temperature Nitriding of Commercially Pure Titanium with Harmonic Structure
British Library Online Contents | 2015
|Laser Gas Nitriding of Titanium and Titanium Alloys
British Library Online Contents | 2009
|The effect of gas nitriding on fatigue behaviour in pure titanium
British Library Online Contents | 1994
|Wear Resistance of VT22 Titanium Alloy After Nitriding Combined with Heat Treatment
British Library Online Contents | 2016
|