A platform for research: civil engineering, architecture and urbanism
Size evolution of the surface short fatigue cracks of 1Cr18Ni9Ti pipe-weld metal with a local viewpoint
Size evolution of the surface short fatigue cracks of 1Cr18Ni9Ti pipe-weld metal with a local viewpoint
Size evolution of the surface short fatigue cracks of 1Cr18Ni9Ti pipe-weld metal with a local viewpoint
Zhao, Y. X. (author)
MATERIALS SCIENCE AND ENGINEERING A ; 344 ; 229-239
2003-01-01
11 pages
Article (Journal)
English
DDC:
620.11
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
British Library Online Contents | 2003
|Density Evolution of the Surface Short Fatigue Cracks of 1Cr18Ni9Ti Pipe-Weld Metal
British Library Online Contents | 2002
|Size Evolution of the Surface Short Fatigue Cracks of 1Cr18Ni9Ti Weld Metal
British Library Online Contents | 2003
|A Short Fatigue Crack Growth Law for 1Cr18Ni9Ti Weld Metal
British Library Online Contents | 2006
|Morphology Evolutions of the Short Fatigue Crack Propagation of 1Cr18Ni9Ti Weld Metal
British Library Online Contents | 2007
|