A platform for research: civil engineering, architecture and urbanism
Study of the Effect of the Indentation Time and Load on Fracture Toughness and Crack Morphologies in WC-17Co Thermally Sprayed HVOF Coating
Study of the Effect of the Indentation Time and Load on Fracture Toughness and Crack Morphologies in WC-17Co Thermally Sprayed HVOF Coating
Study of the Effect of the Indentation Time and Load on Fracture Toughness and Crack Morphologies in WC-17Co Thermally Sprayed HVOF Coating
Asl, S. K. (author) / Sohi, M. H. (author)
MATERIALS SCIENCE FORUM ; 465/466 ; 301-306
2004-01-01
6 pages
Article (Journal)
English
DDC:
620.11
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Study of Phase Transformations in Heat Treatment of HVOF Thermally Sprayed WC-17Co Coating
British Library Online Contents | 2008
|Experimental study of indentation fracture toughness in HVOF sprayed hardmetal coatings
British Library Online Contents | 2013
|Fracture Toughness of HVOF Sprayed Cermet Coatings Measured by Vickers Indentation
British Library Online Contents | 2011
|Fracture toughness and crack morphologies in eroded WC-Co-Cr thermally sprayed coatings
British Library Online Contents | 1998
|British Library Online Contents | 2014
|