Initiation of Environmentally Assisted Cracking in High-Temperature Water
Initiation of Environmentally Assisted Cracking in High-Temperature Water
Initiation of Environmentally Assisted Cracking in High-Temperature Water
Wang, S. (author) / Shoji, T. (author) / Kawaguchi, N. (author)
CORROSION -HOUSTON TX- ; 61 ; 137-144
2005-01-01
8 pages
Article (Journal)
English
DDC:
620.11223