Hydrogen Diffusion in Super 13% Chromium Martensitic Stainless Steel
Hydrogen Diffusion in Super 13% Chromium Martensitic Stainless Steel
Hydrogen Diffusion in Super 13% Chromium Martensitic Stainless Steel
Hinds, G. (author) / Zhao, J. (author) / Griffiths, A. J. (author) / Turnbull, A. (author)
CORROSION -HOUSTON TX- ; 61 ; 348-354
2005-01-01
7 pages
Article (Journal)
English
DDC:
620.11223
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Thermal Fatigue of a 12% Chromium Martensitic Stainless Steel
British Library Online Contents | 1994
|Microstructure and properties of 13Cr5Ni1Mo0.025Nb0.09V0.06N super martensitic stainless steel
British Library Online Contents | 2012
|Role of Nb in low interstitial 13Cr super martensitic stainless steel
British Library Online Contents | 2011
|Corrosion Behavior of Super 13Cr Martensitic Stainless Steel in Live Acid
British Library Online Contents | 2014
|British Library Online Contents | 2013
|