High-temperature tribological properties of Al2O3, Ni-20mass% Cr and NiAl spark-plasma-sintered composites containing BaF2-CaF2 phase
High-temperature tribological properties of Al2O3, Ni-20mass% Cr and NiAl spark-plasma-sintered composites containing BaF2-CaF2 phase
High-temperature tribological properties of Al2O3, Ni-20mass% Cr and NiAl spark-plasma-sintered composites containing BaF2-CaF2 phase
Murakami, T. (author) / Ouyang, J. H. (author) / Sasaki, S. (author) / Umeda, K. (author) / Yoneyama, Y. (author)
WEAR -LAUSANNE- ; 259 ; 626-633
2005-01-01
8 pages
Article (Journal)
English
DDC:
620.11292
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
British Library Online Contents | 2005
|British Library Online Contents | 2004
|Spark-plasma-sintered BaTiO3/Al2O3 nanocomposites
British Library Online Contents | 2003
|British Library Online Contents | 2004
|Spark Plasma Sintered AlN-BN Composites and its Dielectric Properties
British Library Online Contents | 2008
|