Hydrogen damage and delayed fracture in bulk metallic glass
Hydrogen damage and delayed fracture in bulk metallic glass
Hydrogen damage and delayed fracture in bulk metallic glass
Shan, G. B. (author) / Wang, Y. W. (author) / Chu, W. Y. (author) / Li, J. X. (author) / Hui, X. D. (author)
CORROSION SCIENCE ; 47 ; 2731-2739
2005-01-01
9 pages
Article (Journal)
English
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Mechanical Properties, Damage and Fracture Mechanisms of Bulk Metallic Glass Materials
British Library Online Contents | 2007
|Compressive fracture characteristics of Ni42Cu5Ti19Zr22.5Al8Si3.5 bulk metallic glass
British Library Online Contents | 2008
|Fracture behavior of bulk metallic glass/metal laminate composites
British Library Online Contents | 2006
|Mode II fracture behavior of a Zr-based bulk metallic glass
British Library Online Contents | 2006
|Delayed nucleation in Fe40Co40P14B6 metallic glass
British Library Online Contents | 2002
|