A platform for research: civil engineering, architecture and urbanism
High temperature oxidation and erosion-oxidation behaviour of HVOF sprayed Ni-20Cr, WC-20Cr-7Ni and Cr~3C~2-Ni-20Cr coatings
High temperature oxidation and erosion-oxidation behaviour of HVOF sprayed Ni-20Cr, WC-20Cr-7Ni and Cr~3C~2-Ni-20Cr coatings
High temperature oxidation and erosion-oxidation behaviour of HVOF sprayed Ni-20Cr, WC-20Cr-7Ni and Cr~3C~2-Ni-20Cr coatings
Kunioshi, C. T. (author) / Correa, O. V. (author) / Ramanathan, L. V. (author)
SURFACE ENGINEERING -LONDON- ; 22 ; 121-128
2006-01-01
8 pages
Article (Journal)
English
DDC:
620.44
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Oxidation behaviour of micro-crystalline Ni-20Cr-Y2O3 ODS alloy coatings
British Library Online Contents | 2000
|Electrochemical behaviour of Fe-20Cr-5Al and Fe-20Cr-5Al-0.3Y alloys in aqueous solutions
British Library Online Contents | 2008
|Cyclic oxidation behaviour of rare earth oxide coated Fe-20Cr alloys
British Library Online Contents | 2006
|The Effects of Alumina Coatings on the Oxidation of Ni-20Cr
British Library Conference Proceedings | 1996
|Influence of rare earth oxide coatings on oxidation behaviour of Fe-20Cr alloys
British Library Online Contents | 2000
|