Prevention of zinc corrosion in oxygenated 0.5M NaCl by treatment in a cerium(III) nitrate solution and modification with sodium hexadecanoate
Prevention of zinc corrosion in oxygenated 0.5M NaCl by treatment in a cerium(III) nitrate solution and modification with sodium hexadecanoate
Prevention of zinc corrosion in oxygenated 0.5M NaCl by treatment in a cerium(III) nitrate solution and modification with sodium hexadecanoate
Aramaki, K. (author)
CORROSION SCIENCE ; 48 ; 3298-3308
2006-01-01
11 pages
Article (Journal)
English
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
British Library Online Contents | 2006
|The corrosion behaviour of Zr-based bulk metallic glasses in 0.5M NaCl solution
British Library Online Contents | 2011
|Treatment of zinc surface with cerium(III) nitrate to prevent zinc corrosion in aerated 0.5 M NaCl
British Library Online Contents | 2001
|British Library Online Contents | 2016
|British Library Online Contents | 2016
|