Hydrogen degradation of steels in gas mains after long periods of operation
Hydrogen degradation of steels in gas mains after long periods of operation
Hydrogen degradation of steels in gas mains after long periods of operation
Tsyrul’nyk, O. T. (author) / Nykyforchyn, H. M. (author) / Petryna, D. Y. (author) / Hredil’, M. I. (author) / Dz’oba, I. M. (author)