Improvements in fracture properties of Ni-Ti superelastic alloy in physiological saline solution containing hydrogen peroxide by surface modification
Improvements in fracture properties of Ni-Ti superelastic alloy in physiological saline solution containing hydrogen peroxide by surface modification
Improvements in fracture properties of Ni-Ti superelastic alloy in physiological saline solution containing hydrogen peroxide by surface modification
Yokoyama, K. i. (author) / Kanemura, T. (author) / Sakai, J. i. (author)
MATERIALS SCIENCE AND ENGINEERING A ; 513/514 ; 267-275
2009-01-01
9 pages
Article (Journal)
English
DDC:
620.11
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Fracture of nickel-titanium superelastic alloy in sodium hypochlorite solution
British Library Online Contents | 2004
|Hydrogen embrittlement of Ni-Ti superelastic alloy in ethanol solution containing hydrochloric acid
British Library Online Contents | 2005
|Susceptibility to delayed fracture of Ni-Ti superelastic alloy
British Library Online Contents | 2003
|British Library Online Contents | 2003
|