Wear behaviour of low IR-emission titanate ceramics under gross slip fretting conditions against steel and α-alumina
Wear behaviour of low IR-emission titanate ceramics under gross slip fretting conditions against steel and α-alumina
Wear behaviour of low IR-emission titanate ceramics under gross slip fretting conditions against steel and α-alumina
Wäsche, R. (author) / Steinborn, G. (author)
WEAR -LAUSANNE- ; 315 ; 11-16
2014-01-01
6 pages
Article (Journal)
English
DDC:
620.11292
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Shakedown analysis and fretting wear response under gross slip condition
British Library Online Contents | 2001
|Gross slip criteria in fretting
British Library Online Contents | 1993
|Wear of silicon nitride ceramics under fretting conditions
British Library Online Contents | 1996
|British Library Online Contents | 2005
|Friction and wear behaviour of SiAlON ceramics under fretting contacts
British Library Online Contents | 2003
|