Effect of Cathodic Hydrogen Charging Conditions on the Hydrogen Desorption Behavior of the Ni—Ti Superelastic Alloy
Effect of Cathodic Hydrogen Charging Conditions on the Hydrogen Desorption Behavior of the Ni—Ti Superelastic Alloy
Effect of Cathodic Hydrogen Charging Conditions on the Hydrogen Desorption Behavior of the Ni—Ti Superelastic Alloy
Oda, Tetsuro (author) / Ogawa, Toshio (author) / Sakai, Jun-ichi (author)
Corrosion engineering ; 65 ; 138-143
2016-01-01
6 pages
Article (Journal)
English
DDC:
620.11223
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
British Library Online Contents | 2016
|British Library Online Contents | 2008
|Hydrogen embrittlement of Ni-Ti superelastic alloy aged at room temperature after hydrogen charging
British Library Online Contents | 2007
|Effect of cathodic hydrogen charging on the wear behavior of 5754 Al alloy
British Library Online Contents | 2017
|Cathodic hydrogen charging of zinc
British Library Online Contents | 2014
|