Hot corrosion behavior of Al2O3–Cr2O3 refractory by molten glass at 1200°C under static condition
Hot corrosion behavior of Al2O3–Cr2O3 refractory by molten glass at 1200°C under static condition
Hot corrosion behavior of Al2O3–Cr2O3 refractory by molten glass at 1200°C under static condition
Nath, Mithun (author) / Ghosh, A. (author) / Tripathi, H.S. (author)
Corrosion science ; 102 ; 153-160
2016-01-01
8 pages
Article (Journal)
English
DDC:
620.11223
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Hot corrosion behavior of Al2O3–Cr2O3 refractory by molten glass at 1200°C under static condition
British Library Online Contents | 2016
|Hot corrosion behavior of Al2O3–Cr2O3 refractory by molten glass at 1200°C under static condition
British Library Online Contents | 2016
|Al2O3-Cr2O3 refractory aggregate and preparation method thereof
European Patent Office | 2015
|Al2O3-Cr2O3 refractory product taking chrome corundum as aggregate
European Patent Office | 2022
|Hot corrosion behavior of slip-cast alumina-chrome refractory crucible against molten glass
British Library Online Contents | 2014
|