Effects of additive amount, testing method, fabrication process and sintering temperature on the mechanical properties of Al2O3/3Y-TZP composites
Effects of additive amount, testing method, fabrication process and sintering temperature on the mechanical properties of Al2O3/3Y-TZP composites
Effects of additive amount, testing method, fabrication process and sintering temperature on the mechanical properties of Al2O3/3Y-TZP composites
Moradkhani, Alireza (author) / Baharvandi, Hamidreza (author)
Engineering fracture mechanics ; 191 ; 446-460
2018-01-01
15 pages
Article (Journal)
English
DDC:
620.112605
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Fabrication of Al2O3-Ti3SiC2 composites and mechanical properties evaluation
British Library Online Contents | 2003
|Spark plasma sintering and mechanical properties of ZrO2(Y2O3)-Al2O3 composites
British Library Online Contents | 2000
|Fabrication and mechanical properties of SiO2-Al2O3-BNNPs and SiO2-Al2O3-BNNTs composites
British Library Online Contents | 2011
|Microwave sintering and mechanical properties of Y-TZP/20 wt.% Al2O3 composites
British Library Online Contents | 2000
|