A platform for research: civil engineering, architecture and urbanism
Highly porous Fe-2wt%P alloy produced by plasma assisted debinding and sintering of injection-molded parts
Highly porous Fe-2wt%P alloy produced by plasma assisted debinding and sintering of injection-molded parts
Highly porous Fe-2wt%P alloy produced by plasma assisted debinding and sintering of injection-molded parts
Daudt, N.F. (author) / Schütz dos Santos, T.L. (author) / Limberger, I.F. (author) / Seeger, R.L. (author) / Dorneles, L.S. (author) / Binder, C. (author) / Schaeffer, L. (author)
MATERIALS LETTERS ; 231 ; 163-166
2018-01-01
4 pages
Article (Journal)
Unknown
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
Debinding and sintering processes for injection molded pure titanium
British Library Online Contents | 2006
|Plasma Assisted Debinding and Sintering (PADS) - Metal Injection Molding Application
British Library Online Contents | 2006
|Study of the Debinding Rate on MIM Parts Using Plasma Assisted Debinding
British Library Online Contents | 2008
|Effects of debinding parameters on powder injection molded Ti-6Al-4V/HA composite parts
British Library Online Contents | 2001
|A statistical analysis of the factors affecting thermal debinding in powder injection molded parts
British Library Online Contents | 2000
|