Formation of white etching areas in SAE 52100 bearing steel under rolling contact fatigue – Influence of diffusible hydrogen
Formation of white etching areas in SAE 52100 bearing steel under rolling contact fatigue – Influence of diffusible hydrogen
Formation of white etching areas in SAE 52100 bearing steel under rolling contact fatigue – Influence of diffusible hydrogen
Oezel, M. (author) / Schwedt, A. (author) / Janitzky, T. (author) / Kelley, R. (author) / Bouchet-Marquis, C. (author) / Pullan, L. (author) / Broeckmann, C. (author) / Mayer, J. (author)
Wear = ; 414 ; 352-365
2018-01-01
14 pages
Article (Journal)
English
DDC:
621.89
© Metadata Copyright the British Library Board and other contributors. All rights reserved.
British Library Online Contents | 2013
|British Library Online Contents | 2017
|British Library Online Contents | 2017
|Rolling Contact Fatigue of White Etching Layer on Pearlite Steel Rail
British Library Online Contents | 2010
|Rolling-contact fatigue lives of steel AISI 52100 balls with eight mineral and synthetic lubricants
British Library Online Contents | 1996
|