The Submicron Grinding of BaTiO3 by Ball Milling [Translated]†
The submicron grinding of BaTiO3 powder was studied by a ball mill with small alumina balls of 0.75 mmΦ to 30 mmΦ. BaTiO3 clinker, which was obtained by calcining an equimolar mixture of TiO2 and BaCO3, was preground to 1.8 micron. Submicron grinding of the BaTiO3 powder was possible by ball milling with several mmΦ balls. For a ball diameter of 2 mm, the specific surface area was maximized.An attempt was made to represent the specific surface area in terms of volume per ball and total surface area of used balls, and the following experimental equation with a time term was obtained,In(SS) = -0.247lnr3 - 0.738/r + 0.429 lnt + 1.57where SS is the specific surface area, r is the ball radius, and t is time. The multiple correlation coefficient R was found to be 0.982 when calculated by computer.† This report was originally printed in J. Soc. Materials Science, Japan, 35(388), 54-58 (1986) in Japanese, before being translated into English by KONA Editorial Committee with the permission of the editorial committee of the Soc. Materials Science, Japan.
The Submicron Grinding of BaTiO3 by Ball Milling [Translated]†
The submicron grinding of BaTiO3 powder was studied by a ball mill with small alumina balls of 0.75 mmΦ to 30 mmΦ. BaTiO3 clinker, which was obtained by calcining an equimolar mixture of TiO2 and BaCO3, was preground to 1.8 micron. Submicron grinding of the BaTiO3 powder was possible by ball milling with several mmΦ balls. For a ball diameter of 2 mm, the specific surface area was maximized.An attempt was made to represent the specific surface area in terms of volume per ball and total surface area of used balls, and the following experimental equation with a time term was obtained,In(SS) = -0.247lnr3 - 0.738/r + 0.429 lnt + 1.57where SS is the specific surface area, r is the ball radius, and t is time. The multiple correlation coefficient R was found to be 0.982 when calculated by computer.† This report was originally printed in J. Soc. Materials Science, Japan, 35(388), 54-58 (1986) in Japanese, before being translated into English by KONA Editorial Committee with the permission of the editorial committee of the Soc. Materials Science, Japan.
The Submicron Grinding of BaTiO3 by Ball Milling [Translated]†
Kenji Tanaka (author) / Kiichi Minai (author) / Kikuo Wakino (author) / Isao Uei (author)
2014
Article (Journal)
Electronic Resource
Unknown
Metadata by DOAJ is licensed under CC BY-SA 1.0
Synthesis of BaTiO3 powders by a ball milling-assisted hydrothermal reaction
British Library Online Contents | 2008
|Preparation of porous BaTiO3-based ceramics by high-energy ball-milling process
British Library Online Contents | 2006
|Grinding Process of Ball End Milling Cutter Flank
British Library Online Contents | 2018
|Submicron-Structured Al Matrix Composite by Ball-Milling and Hot-Extruding Techniques
British Library Online Contents | 2006
|