Strength properties of slag/fly ash blends activated with sodium metasilicate
The alkali activation of mortar blends containing Ground Granulated Blast Furnace Slag and Fly Ash, with activation based on sodium metasilicate, is investigated in this study. Two series are investigated, and compressive strength is measured. The results of the first series show that the compressive strength decreases considerably with a decrease in the slag and fly ash ratio. The 3-day compressive strength of mortar cured at the temperature of 100°C increases slightly up to the ratio of 60/40, but decreases considerably at the 40/60 ratio.
Strength properties of slag/fly ash blends activated with sodium metasilicate
The alkali activation of mortar blends containing Ground Granulated Blast Furnace Slag and Fly Ash, with activation based on sodium metasilicate, is investigated in this study. Two series are investigated, and compressive strength is measured. The results of the first series show that the compressive strength decreases considerably with a decrease in the slag and fly ash ratio. The 3-day compressive strength of mortar cured at the temperature of 100°C increases slightly up to the ratio of 60/40, but decreases considerably at the 40/60 ratio.
Strength properties of slag/fly ash blends activated with sodium metasilicate
Erion Luga (author) / Cengiz Duran Atis (author) / Okan Karahan (author) / Serhan Ilkentapar (author) / Ela Bahsude Gorur (author)
2017
Article (Journal)
Electronic Resource
Unknown
Metadata by DOAJ is licensed under CC BY-SA 1.0
DOAJ | 2018
|Preparation method of ceramic deflocculant-sodium metasilicate
European Patent Office | 2023
|