Casting ingot mold stools in chill molds
Casting stools in split metal molds covered with layer of paint 2-3 mm thick results in significantly increased stool life compared with sand cast variety; considerable increase in productivity noted; silicon content of iron should be raised (2.0-2.2% with 3.5-3.7% C). (See also Stal n 2 Feb 1963 p 185-7)
Casting ingot mold stools in chill molds
Casting stools in split metal molds covered with layer of paint 2-3 mm thick results in significantly increased stool life compared with sand cast variety; considerable increase in productivity noted; silicon content of iron should be raised (2.0-2.2% with 3.5-3.7% C). (See also Stal n 2 Feb 1963 p 185-7)
Casting ingot mold stools in chill molds
Otlivka poddonov dlya izlozhnits v kokil'nykh formakh
Krasovitskii, V.S. (author) / Turchenkova, E.K. (author) / Egnus, R.M. (author)
1963
2 pages
Article (Journal)
English
© Metadata Copyright Elsevier B. V. All rights reserved.
Casting ingot mold stools in chill molds
Engineering Index Backfile | 1963
|Direct Chill Casting of CLAD Ingot
British Library Online Contents | 2006
|Hot tearing in direct chill casting ingot of 7000 series aluminum alloys
British Library Online Contents | 2015
|New method of preparing casting molds and mold cores
Engineering Index Backfile | 1959
|New method of preparing casting molds and mold cores
Engineering Index Backfile | 1959
|