Fifteen-year exposure test of porcelain enamels
Weather resistance of 768 panels representing 14 types of enamel evaluated at Washington, DC, St Louis, Mo, Lakeland, Fla, and Atlantic City, NJ; changes in gloss and color taken as criteria of resistance; results for ease of cleaning, corrosion protection, gloss, color difference, microstructure of surface, and effect of variation of conditions at four sites.
Fifteen-year exposure test of porcelain enamels
Weather resistance of 768 panels representing 14 types of enamel evaluated at Washington, DC, St Louis, Mo, Lakeland, Fla, and Atlantic City, NJ; changes in gloss and color taken as criteria of resistance; results for ease of cleaning, corrosion protection, gloss, color difference, microstructure of surface, and effect of variation of conditions at four sites.
Fifteen-year exposure test of porcelain enamels
U S Bur Standards -- Bldg Matls Structures Report
Moore, D.G. (author) / Harrison, W.N. (author)
1957
13 pages
Report
English