Washington airport runways use local aggregates for asphalt pavement
Design, construction and costs of 450,000 sq yd of 3 1/2-in. hot mixed asphaltic concrete hot laid in two courses on runways, main taxiways and aprons of National Airport at Washington, DC; aggregates supply; aggregate plant; aggregate gradation; mineral filler gradation; mixer design; asphalt storage; truck handling; paving equipment. (p 42-4, 80, 82-3, 84, 86, 88, 90)
Washington airport runways use local aggregates for asphalt pavement
Design, construction and costs of 450,000 sq yd of 3 1/2-in. hot mixed asphaltic concrete hot laid in two courses on runways, main taxiways and aprons of National Airport at Washington, DC; aggregates supply; aggregate plant; aggregate gradation; mineral filler gradation; mixer design; asphalt storage; truck handling; paving equipment. (p 42-4, 80, 82-3, 84, 86, 88, 90)
Washington airport runways use local aggregates for asphalt pavement
Construction Methods
1940
Article (Journal)
English
© Metadata Copyright Elsevier B. V. All rights reserved.
Engineering Index Backfile | 1930
|Engineering Index Backfile | 1930
|Engineering Index Backfile | 1929
|Runways for Washington national airport
Engineering Index Backfile | 1941
|Runways for Washington National Airport
Engineering Index Backfile | 1940