Causes of hair-crack formations in cast-iron enameled ware
Expansion of enamel taking into consideration expansion of both enamel and iron in relation to temperature up to softening point of enamel.
Causes of hair-crack formations in cast-iron enameled ware
Expansion of enamel taking into consideration expansion of both enamel and iron in relation to temperature up to softening point of enamel.
Causes of hair-crack formations in cast-iron enameled ware
Ueber die Ursachen der Haarrissebildung bei Eisenmail
Weinig, R. (author)
1930
2 pages
3 Figs.
Article (Journal)
German
© Metadata Copyright Elsevier B. V. All rights reserved.
Fire brick, glazed ware, an enameled ware improved by study of manufacturing methods
Engineering Index Backfile | 1929
|Lead poisoning in potteries, file works, and porcelain enameled sanitary ware factories
Engineering Index Backfile | 1912
|Engineering Index Backfile | 1957
|Porcelain enameled iron and its relation to sanitation
Engineering Index Backfile | 1913
|Engineering Index Backfile | 1940
|