Effect of deoxidation by silicocalcium on properties of Cr-Ni-Mo steel
Results of investigations presented; when aluminum is replaced by silicocalcium equivalent to 0.15% Ca for final deoxidation of steel it is possible to obtain castings free from surface porosity and having improved ductile and impact properties. (See also Stal v 19 n 10 Oct 1959 p 938-41)
Effect of deoxidation by silicocalcium on properties of Cr-Ni-Mo steel
Results of investigations presented; when aluminum is replaced by silicocalcium equivalent to 0.15% Ca for final deoxidation of steel it is possible to obtain castings free from surface porosity and having improved ductile and impact properties. (See also Stal v 19 n 10 Oct 1959 p 938-41)
Effect of deoxidation by silicocalcium on properties of Cr-Ni-Mo steel
Vliyanie raskisleniya silikokal'tsiem na svoistva khromonikel'molibdenovoi stali
Verbol'Skaya, E.D. (author) / Khlebnikov, A.E. (author) / Smolenskii, S.I. (author)
1959
4 pages
Article (Journal)
English
© Metadata Copyright Elsevier B. V. All rights reserved.
Effect of deoxidation by silicocalcium on properties of Cr-Ni-Mo steel
Engineering Index Backfile | 1959
|Process of producing magnesium by thermal vacuum reduction using silicocalcium as reductant
British Library Online Contents | 2016
|Desulphurization and deoxidation of steel melts
Engineering Index Backfile | 1956
|Additions of aluminium for deoxidation of steel
Engineering Index Backfile | 1967
|Preliminary deoxidation and hydrogen content in steel
Engineering Index Backfile | 1959
|