HIGH PERFORMANCE SULFO-ALUMINOUS CLINKER
The invention relates to a sulfo-aluminous clinker with optimal setting time and short term compressive strengths, comprising a mixture of the following phases: - calcium sulfoaluminate, or C4A3$, in amounts higher than 50 % by weight of the mixture, - belite, or C2S, in amounts between 2 and 23%, - 3C2S 3C$ CaX2, X being fluorine or chlorine, between 3 and 15% - C11A7CaX2, X being fluorine or chlorine, between 2 and 12%, both fluorine and chlorine being altogether present in the mixture, and phase C5S2$ being absent. The invention also relates to a method for preparing this sulfo-aluminous clinker, and hydraulic binders comprising this clinker.
Cette invention concerne un clinker sulfo-alumineux ayant un temps de prise optimal et des contraintes en compression à court terme également optimales, ledit clinker sulfo-alumineux comprenant un mélange des phases suivantes : sulfoaluminate de calcium, or C4A3S, en des quantités supérieures à 50 % en poids du mélange, - bélite, ou C2S, en des quantités entre 2 et 23 %, - 3C2S 3C$ CaX2, X étant un atome de fluor ou de chlore, entre 3 et 15 %, - C11A7CaX2, X étant un atome de fluor ou de chlore, entre 2 et 12 %, le fluor et le chlore étant tous deux présents ensemble dans le mélange, et la phase C5S2S étant absente. Cette invention concerne également un procédé de préparation de ce clinker sulfo-alumineux, et des liants hydrauliques le contenant.
HIGH PERFORMANCE SULFO-ALUMINOUS CLINKER
The invention relates to a sulfo-aluminous clinker with optimal setting time and short term compressive strengths, comprising a mixture of the following phases: - calcium sulfoaluminate, or C4A3$, in amounts higher than 50 % by weight of the mixture, - belite, or C2S, in amounts between 2 and 23%, - 3C2S 3C$ CaX2, X being fluorine or chlorine, between 3 and 15% - C11A7CaX2, X being fluorine or chlorine, between 2 and 12%, both fluorine and chlorine being altogether present in the mixture, and phase C5S2$ being absent. The invention also relates to a method for preparing this sulfo-aluminous clinker, and hydraulic binders comprising this clinker.
Cette invention concerne un clinker sulfo-alumineux ayant un temps de prise optimal et des contraintes en compression à court terme également optimales, ledit clinker sulfo-alumineux comprenant un mélange des phases suivantes : sulfoaluminate de calcium, or C4A3S, en des quantités supérieures à 50 % en poids du mélange, - bélite, ou C2S, en des quantités entre 2 et 23 %, - 3C2S 3C$ CaX2, X étant un atome de fluor ou de chlore, entre 3 et 15 %, - C11A7CaX2, X étant un atome de fluor ou de chlore, entre 2 et 12 %, le fluor et le chlore étant tous deux présents ensemble dans le mélange, et la phase C5S2S étant absente. Cette invention concerne également un procédé de préparation de ce clinker sulfo-alumineux, et des liants hydrauliques le contenant.
HIGH PERFORMANCE SULFO-ALUMINOUS CLINKER
CLINKER SULFO-ALUMINEUX HAUTE PERFORMANCE
MARCHI MAURIZIO ILER (author) / ALLEVI STEFANO (author)
2018-11-13
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2019
|European Patent Office | 2015
|