Thermal-insulation anti-cracking impervious concrete
Related thermal-insulation anti-cracking impervious concrete comprises the following compositions in parts by weight: 500-600 parts of cement, 30-45 parts of fine aggregate sand, 20-30 parts of crude aggregate cobblestone, 10-20 parts of a foaming agent, and 300-400 parts of water. The thermal-insulation anti-cracking impervious concrete employing the above design scheme has good thermal insulation performance and can possess warm-keeping effect.
Thermal-insulation anti-cracking impervious concrete
Related thermal-insulation anti-cracking impervious concrete comprises the following compositions in parts by weight: 500-600 parts of cement, 30-45 parts of fine aggregate sand, 20-30 parts of crude aggregate cobblestone, 10-20 parts of a foaming agent, and 300-400 parts of water. The thermal-insulation anti-cracking impervious concrete employing the above design scheme has good thermal insulation performance and can possess warm-keeping effect.
Thermal-insulation anti-cracking impervious concrete
LIU JINGLAN (author)
2015-04-08
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Environment-friendly anti-cracking thermal insulation concrete
European Patent Office | 2020
|European Patent Office | 2024
|Engineering Index Backfile | 1903