CoFe2O4/BaTiO3-(Na0.5Bi0.5)TiO3 material and preparation method thereof
The invention discloses a CoFe2O4/BaTiO3-(Na0.5Bi0.5)TiO3 material and a preparation method thereof. The preparation method comprises the following steps: preparing 0.65BaTiO3-0.35(Na0.5Bi0.5)TiO3 powder with barium carbonate, titania, bismuth oxide and sodium carbonate as raw materials, carrying out granulation on CoFe2O4 powder and the 0.65BaTiO3-0.35(Na0.5Bi0.5)TiO3 powder, carrying out compression moulding in a die according to a 2-2 compounding layering staking arrangement mode, discharging rubber, and calcining. According to the CoFe2O4/BaTiO3-(Na0.5Bi0.5)TiO3 material and the preparation method thereof disclosed by the invention, as a ferroelectric phase and a ferromagnetic phase are co-fired together in a layering compounding mode according to the 2-2 compounding layering staking arrangement mode, mutual reaction between the ferroelectric phase and the ferromagnetic phase can be effectively inhibited so as to keep respective characteristics, and the CoFe2O4/BaTiO3-(Na0.5Bi0.5)TiO3 material is good in both ferroelectricity and ferromagnetism.
CoFe2O4/BaTiO3-(Na0.5Bi0.5)TiO3 material and preparation method thereof
The invention discloses a CoFe2O4/BaTiO3-(Na0.5Bi0.5)TiO3 material and a preparation method thereof. The preparation method comprises the following steps: preparing 0.65BaTiO3-0.35(Na0.5Bi0.5)TiO3 powder with barium carbonate, titania, bismuth oxide and sodium carbonate as raw materials, carrying out granulation on CoFe2O4 powder and the 0.65BaTiO3-0.35(Na0.5Bi0.5)TiO3 powder, carrying out compression moulding in a die according to a 2-2 compounding layering staking arrangement mode, discharging rubber, and calcining. According to the CoFe2O4/BaTiO3-(Na0.5Bi0.5)TiO3 material and the preparation method thereof disclosed by the invention, as a ferroelectric phase and a ferromagnetic phase are co-fired together in a layering compounding mode according to the 2-2 compounding layering staking arrangement mode, mutual reaction between the ferroelectric phase and the ferromagnetic phase can be effectively inhibited so as to keep respective characteristics, and the CoFe2O4/BaTiO3-(Na0.5Bi0.5)TiO3 material is good in both ferroelectricity and ferromagnetism.
CoFe2O4/BaTiO3-(Na0.5Bi0.5)TiO3 material and preparation method thereof
YANG HAIBO (author) / ZHANG GE (author) / LIN YING (author) / ZHU JIANFENG (author) / WANG FEN (author)
2015-04-29
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Synthesis of (Na0.5Bi0.5)TiO3 and (Na0.5Bi0.5)0.92Ba0.08TiO3 powders by a citrate method
British Library Online Contents | 2006
|British Library Online Contents | 2011
|CoFe2O4/BaTiO3 layered magnetoelectric composite material and preparation method thereof
European Patent Office | 2015
|Dielectric and piezoelecrtic properties of lead-free (Na0.5Bi0.5)TiO3-NaNbO3 ceramics
British Library Online Contents | 2004
|Synthesis, ferroelectric and piezoelectric properties of some (Na0.5Bi0.5)TiO3 system compositions
British Library Online Contents | 2005
|