Preparation method for colorful polyurethane plastic and construction process for colorful polyurethane plastic track
The invention discloses a preparation method and a construction process for a colorful polyurethane plastic track, and belongs to the technical field of sports facilities. The preparation method for colorful polyurethane plastic comprises the following steps: uniformly stirring 10 to 15 parts of polyether polyol, 10 to 30 parts of hydroxylated acrylic resin, 10 to 30 parts of paraffin, 2 to 4 parts of a chain extender and 0.1 to 0.5 part of an age resistor, and raising temperature to 90 to 100 DEG C; adding 30 to 50 parts of a filler, 2 to 9 parts of a pigment and 0.1 to 0.5 parts of an age resistor, and performing uniform stirring; starting a colloid grinder to grind the materials into particle sizes of smaller than 400 meshes; continuing heating, and performing dehydration for 2 to 3 hours under the conditions of temperature of 90 to 100 DEG C and vacuum degree of lower than 0.095Mpa. According to the preparation method and the construction process, with the adoption of the high-functionality polyether polyol, reaction is accelerated, the hardness of a formed film is increased, and construction time is shortened; by the hydroxylated acrylic resin, high glossiness and higher weather resistance and color retention are achieved, and the service life is prolonged.
Preparation method for colorful polyurethane plastic and construction process for colorful polyurethane plastic track
The invention discloses a preparation method and a construction process for a colorful polyurethane plastic track, and belongs to the technical field of sports facilities. The preparation method for colorful polyurethane plastic comprises the following steps: uniformly stirring 10 to 15 parts of polyether polyol, 10 to 30 parts of hydroxylated acrylic resin, 10 to 30 parts of paraffin, 2 to 4 parts of a chain extender and 0.1 to 0.5 part of an age resistor, and raising temperature to 90 to 100 DEG C; adding 30 to 50 parts of a filler, 2 to 9 parts of a pigment and 0.1 to 0.5 parts of an age resistor, and performing uniform stirring; starting a colloid grinder to grind the materials into particle sizes of smaller than 400 meshes; continuing heating, and performing dehydration for 2 to 3 hours under the conditions of temperature of 90 to 100 DEG C and vacuum degree of lower than 0.095Mpa. According to the preparation method and the construction process, with the adoption of the high-functionality polyether polyol, reaction is accelerated, the hardness of a formed film is increased, and construction time is shortened; by the hydroxylated acrylic resin, high glossiness and higher weather resistance and color retention are achieved, and the service life is prolonged.
Preparation method for colorful polyurethane plastic and construction process for colorful polyurethane plastic track
LU LING (author) / ZHANG ZHEN (author) / LI SHUAI (author)
2015-06-17
Patent
Electronic Resource
English
IPC:
C08G
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONS ONLY INVOLVING CARBON-TO-CARBON UNSATURATED BONDS
,
Makromolekulare Verbindungen, anders erhalten als durch Reaktionen, an denen nur ungesättigte Kohlenstoff-Kohlenstoff-Bindungen beteiligt sind
/
C09D
Überzugsmittel, z.B. Anstrichstoffe, Firnisse oder Lacke
,
COATING COMPOSITIONS, e.g. PAINTS, VARNISHES OR LACQUERS
/
E01C
Bau von Straßen, Sportplätzen oder dgl., Decken dafür
,
CONSTRUCTION OF, OR SURFACES FOR, ROADS, SPORTS GROUNDS, OR THE LIKE
Colorful prefabricated polyurethane micro-foaming runway material and preparation method thereof
European Patent Office | 2023
|Anti-yellowing colorful polyurethane adhesive stone permeable pavement material
European Patent Office | 2021
|