Steam-curing-free early-strength steel fiber concrete pipe segment and preparation method thereof
The invention discloses a steam-curing-free early-strength steel fiber concrete pipe segment comprising ordinary Portland cement, early-strength sulphoaluminate cement, fly ash, slag, fine aggregate, coarse aggregate, water, a polycarboxylic acid type water reducer and end hook type steel fibers. The invention also discloses a preparation method of the steam-curing-free early-strength steel fiber concrete pipe segment. The steam-curing-free early-strength steel fiber concrete pipe segment is quick in coagulation and hardening and high in early strength, can reach the strength of 15MPa required by pipe segment demolding in 6-8 hours, and can be prepared into a concrete pipe segment for an underground structure by performing water curing in a 20 DEG C saturated calcium hydroxide solution for 24 hours and then performing natural curing for 28 days. The steam-curing-free early-strength steel fiber concrete pipe segment does not need steam curing, so that the curing mode of the pipe segment can be simplified, the curing time is shortened, a lot of manpower and resources are saved, and the popularization and application values are high.
Steam-curing-free early-strength steel fiber concrete pipe segment and preparation method thereof
The invention discloses a steam-curing-free early-strength steel fiber concrete pipe segment comprising ordinary Portland cement, early-strength sulphoaluminate cement, fly ash, slag, fine aggregate, coarse aggregate, water, a polycarboxylic acid type water reducer and end hook type steel fibers. The invention also discloses a preparation method of the steam-curing-free early-strength steel fiber concrete pipe segment. The steam-curing-free early-strength steel fiber concrete pipe segment is quick in coagulation and hardening and high in early strength, can reach the strength of 15MPa required by pipe segment demolding in 6-8 hours, and can be prepared into a concrete pipe segment for an underground structure by performing water curing in a 20 DEG C saturated calcium hydroxide solution for 24 hours and then performing natural curing for 28 days. The steam-curing-free early-strength steel fiber concrete pipe segment does not need steam curing, so that the curing mode of the pipe segment can be simplified, the curing time is shortened, a lot of manpower and resources are saved, and the popularization and application values are high.
Steam-curing-free early-strength steel fiber concrete pipe segment and preparation method thereof
GUO LIPING (author) / DING CONG (author)
2015-07-15
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Steam-free self-curing concrete pipe pile and preparation method thereof
European Patent Office | 2022
|European Patent Office | 2021
|Steam-curing-free super-early-strength C120 self-compacting concrete and preparation method thereof
European Patent Office | 2024
|Steam-curing-free concrete and preparation method thereof
European Patent Office | 2021
|Steam-curing-free high-strength anti-corrosion pipe pile and preparation method thereof
European Patent Office | 2021
|