(BN/SiC)n composite interface-phase coating, coating fiber and preparation method
The invention discloses a (BN/SiC)n composite interface-phase coating. The (BN/SiC)n composite interface-phase coating has a periodic laminated structure, wherein BN layers and SiC layers are alternatively and periodically overlapped; the thickness of the BN layers is not greater than that of the SiC layer. A coating fiber comprises a fiber substrate and the (BN/SiC)n composite interface-phase coating; the innermost layer closest to the fiber substrate is the NB layer and the outermost layer further away from the fiber substrate is the SiC layer. A preparation method for the coating fiber comprises the steps: cleaning the fiber substrate; putting into a deposition hearth, vacuumizing and filling with inert gases to exchange with air; realizing a preset vacuum degree and a preset temperature; bringing precursors into the reaction by carrier gas in a bubbling manner, maintaining a specified pressure of a reaction system, and alternatively depositing the BN layers and the SiC layers on the fiber substrate through changing a precursor gas source. The product has the advantages of good compatibility, high-temperature resistance, anti-oxidation and good toughening effect.
(BN/SiC)n composite interface-phase coating, coating fiber and preparation method
The invention discloses a (BN/SiC)n composite interface-phase coating. The (BN/SiC)n composite interface-phase coating has a periodic laminated structure, wherein BN layers and SiC layers are alternatively and periodically overlapped; the thickness of the BN layers is not greater than that of the SiC layer. A coating fiber comprises a fiber substrate and the (BN/SiC)n composite interface-phase coating; the innermost layer closest to the fiber substrate is the NB layer and the outermost layer further away from the fiber substrate is the SiC layer. A preparation method for the coating fiber comprises the steps: cleaning the fiber substrate; putting into a deposition hearth, vacuumizing and filling with inert gases to exchange with air; realizing a preset vacuum degree and a preset temperature; bringing precursors into the reaction by carrier gas in a bubbling manner, maintaining a specified pressure of a reaction system, and alternatively depositing the BN layers and the SiC layers on the fiber substrate through changing a precursor gas source. The product has the advantages of good compatibility, high-temperature resistance, anti-oxidation and good toughening effect.
(BN/SiC)n composite interface-phase coating, coating fiber and preparation method
CHENG HAIFENG (author) / LI JUNSHENG (author) / LI BIN (author) / LIU HAITAO (author) / ZHOU YONGJIANG (author) / TONG SICHAO (author) / ZHANG CHAOYANG (author) / ZHENG WENWEI (author)
2015-08-05
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
C/(SiC/BN)n compound interface phase coating, coating fiber and preparation method of coating fiber
European Patent Office | 2015
|European Patent Office | 2020
|Preparation method of TiSiBN interface coating on surface of ceramic fiber
European Patent Office | 2023
|FIBER HAVING INTEGRAL WEAK INTERFACE COATING, METHOD OF MAKING AND COMPOSITE INCORPORATING THE FIBER
European Patent Office | 2023
|Fiber having integral weak interface coating, method of making and composite incorporating the fiber
European Patent Office | 2022
|