Environmentally-friendly tourmaline autoclaved brick
The invention discloses an environmentally-friendly tourmaline autoclaved brick which is made of the following raw materials in parts by weight: 8-12parts of cement, 5-7 parts of tourmaline powders, 4-8 parts of expanded vermiculite powders, 1-3 parts of iron mine tailing powders, 4-8 parts of coal ashes, 6-8 parts of causticized white mud, 5- 10 parts of river sands, 2-4 parts of titanium dioxides, 1-2 parts of aluminium nitrate, 1-2 parts of magnesium nitrate, 0.2-0.3 parts of azobisformamide, 0.1-0.2 parts of ammonium persulfate, 0.2-0.4 parts of carbomer, 0.1-0.2 parts of polyacrylic acid, 0.1-0.3 parts of stearic acid and appropriate amount of deionized water.
Environmentally-friendly tourmaline autoclaved brick
The invention discloses an environmentally-friendly tourmaline autoclaved brick which is made of the following raw materials in parts by weight: 8-12parts of cement, 5-7 parts of tourmaline powders, 4-8 parts of expanded vermiculite powders, 1-3 parts of iron mine tailing powders, 4-8 parts of coal ashes, 6-8 parts of causticized white mud, 5- 10 parts of river sands, 2-4 parts of titanium dioxides, 1-2 parts of aluminium nitrate, 1-2 parts of magnesium nitrate, 0.2-0.3 parts of azobisformamide, 0.1-0.2 parts of ammonium persulfate, 0.2-0.4 parts of carbomer, 0.1-0.2 parts of polyacrylic acid, 0.1-0.3 parts of stearic acid and appropriate amount of deionized water.
Environmentally-friendly tourmaline autoclaved brick
WANG CHANGFU (author) / MAO DONGCHAO (author) / WANG YUTONG (author) / LIU WEI (author)
2015-08-19
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Preparation method of environment-friendly autoclaved coal gangue brick
European Patent Office | 2021
|Fly ash autoclaved environment-friendly brick and preparation method thereof
European Patent Office | 2021
|