Preparation method of self-lubricating ceramic cutting tool material comprising spherical nanometer silicon dioxide coated hexagonal boron nitride composite powder
The invention relates to a preparation method of self-lubricating ceramic cutting tool material comprising spherical nanometer silicon dioxide coated hexagonal boron nitride composite powder. The self-lubricating ceramic cutting tool material comprises the following raw material components in percentage by volume: 15-75% of TiC, 2-20% of h-BN@SiO2, 0.2-2.5% of MgO and the balance of Al2O3, wherein the h-BN@SiO2 is the spherical silicon dioxide coated hexagonal boron nitride composite powder which is obtained by dispersing h-BN powder in absolute ethyl alcohol and dropwise adding tetraethyl orthosilicate at the temperature of 30-70 DEG C. The invention also provides the preparation method of the self-lubricating ceramic cutting tool material. The added h-BN@SiO2 can improve the wettability of h-BN@SiO2 and a matrix and the mechanical property of the cutting tool material when the excellent lubricating property of the cutting tool material is remained, and reduce the agglomeration of air holes and the h-BN@SiO2 and the negative influence of the added h-BN on the mechanical property of the self-lubricating ceramic cutting tool material. The self-lubricating ceramic cutting tool material is suitable for application in manufacturing of self-lubricating ceramic cutting tools and can also be used for manufacturing ceramic molds, bearings and other wear-resisting anti-corrosion components and parts.
Preparation method of self-lubricating ceramic cutting tool material comprising spherical nanometer silicon dioxide coated hexagonal boron nitride composite powder
The invention relates to a preparation method of self-lubricating ceramic cutting tool material comprising spherical nanometer silicon dioxide coated hexagonal boron nitride composite powder. The self-lubricating ceramic cutting tool material comprises the following raw material components in percentage by volume: 15-75% of TiC, 2-20% of h-BN@SiO2, 0.2-2.5% of MgO and the balance of Al2O3, wherein the h-BN@SiO2 is the spherical silicon dioxide coated hexagonal boron nitride composite powder which is obtained by dispersing h-BN powder in absolute ethyl alcohol and dropwise adding tetraethyl orthosilicate at the temperature of 30-70 DEG C. The invention also provides the preparation method of the self-lubricating ceramic cutting tool material. The added h-BN@SiO2 can improve the wettability of h-BN@SiO2 and a matrix and the mechanical property of the cutting tool material when the excellent lubricating property of the cutting tool material is remained, and reduce the agglomeration of air holes and the h-BN@SiO2 and the negative influence of the added h-BN on the mechanical property of the self-lubricating ceramic cutting tool material. The self-lubricating ceramic cutting tool material is suitable for application in manufacturing of self-lubricating ceramic cutting tools and can also be used for manufacturing ceramic molds, bearings and other wear-resisting anti-corrosion components and parts.
Preparation method of self-lubricating ceramic cutting tool material comprising spherical nanometer silicon dioxide coated hexagonal boron nitride composite powder
XU CHONGHAI (author) / CHEN HUI (author) / YI MINGDONG (author) / XIAO GUANGCHUN (author) / CHEN ZHAOQIANG (author) / MA JUN (author)
2015-08-19
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
European Patent Office | 2015
|European Patent Office | 2015
|European Patent Office | 2015
|European Patent Office | 2022
|European Patent Office | 2021
|