A platform for research: civil engineering, architecture and urbanism
Energy-saving building material and preparation method thereof
The invention discloses an energy-saving building material and a preparation method thereof. The energy-saving building material comprises the following components in parts by weight: 8-22 parts of sea-foam stone powder, 6-17 parts of bentonite, 5-15 parts of ethylene propylene diene monomer, 11-18 parts of coal ash, 9-20 parts of tetra calcium aluminoferrite, 6-14 parts of calcium hypophosphite, 5-11 parts of zinc borate, 3-8 parts of nanosilicon dioxide, and 5-9 parts of aluminum silicate wool. The preparation method comprises the following steps of: (1) respectively grinding sea-foam stone powder, bentonite, coal ash, tetra calcium aluminoferrite, calcium hypophosphite, zinc borate and nanosilicon dioxide by using a grinding machine so as to respectively obtain powder of the above components; (2) opening a high-speed dispersion machine, and adding the above components into the high-speed dispersion machine to mix; and (3) pressurizing the mixed building material in a high-temperature mould, pressing at high temperature, and taking out from the mould after pressing so as to obtain the energy-saving building material.
Energy-saving building material and preparation method thereof
The invention discloses an energy-saving building material and a preparation method thereof. The energy-saving building material comprises the following components in parts by weight: 8-22 parts of sea-foam stone powder, 6-17 parts of bentonite, 5-15 parts of ethylene propylene diene monomer, 11-18 parts of coal ash, 9-20 parts of tetra calcium aluminoferrite, 6-14 parts of calcium hypophosphite, 5-11 parts of zinc borate, 3-8 parts of nanosilicon dioxide, and 5-9 parts of aluminum silicate wool. The preparation method comprises the following steps of: (1) respectively grinding sea-foam stone powder, bentonite, coal ash, tetra calcium aluminoferrite, calcium hypophosphite, zinc borate and nanosilicon dioxide by using a grinding machine so as to respectively obtain powder of the above components; (2) opening a high-speed dispersion machine, and adding the above components into the high-speed dispersion machine to mix; and (3) pressurizing the mixed building material in a high-temperature mould, pressing at high temperature, and taking out from the mould after pressing so as to obtain the energy-saving building material.
Energy-saving building material and preparation method thereof
YAO CHUNLONG (author)
2015-09-02
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME
Energy-saving building material and preparation method thereof
European Patent Office | 2021
|Energy-saving building wall material and preparation method thereof
European Patent Office | 2022
|Green energy-saving building material and preparation method thereof
European Patent Office | 2020
|Building energy-saving thermal insulation material and preparation method thereof
European Patent Office | 2023
|Building energy-saving thermal insulation material and preparation method thereof
European Patent Office | 2020
|