Waterproofing slurry is prepared from the following materials in parts by weight: 15 to 26 parts of fumed silica, 2 to 4 parts of a defoamer, 25 to 24 parts of 80 to 120 mesh aggregate, 2 to 4 parts of rubber powder, 2 to 5 parts of stannic oxide, 8 to 20 parts of polyester acrylate, 0.6 to 1 part of acetic acid-dissolved chitosan, 1.2 to 2parts of a fiber additive, 0.5 to 1 part of coconut oil, 0.6 to 1.2 parts of dispersible rubber powder, 10 to 16 parts of fatty acid triglyceride, 0.6 to 1 part of a Ca-Zn composite heat stabilizer, 4 to 10 parts of a carbide, 5 to 9 parts of sodium nitrite and 8 to 12 parts of a coupling agent. The waterproofing slurry has the beneficial effects of being capable of well bonding with a base surface, difficult to fall, short in curing drying time, and excellent in mildew resistance, weatherability and waterproofness.
Waterproofing slurry is prepared from the following materials in parts by weight: 15 to 26 parts of fumed silica, 2 to 4 parts of a defoamer, 25 to 24 parts of 80 to 120 mesh aggregate, 2 to 4 parts of rubber powder, 2 to 5 parts of stannic oxide, 8 to 20 parts of polyester acrylate, 0.6 to 1 part of acetic acid-dissolved chitosan, 1.2 to 2parts of a fiber additive, 0.5 to 1 part of coconut oil, 0.6 to 1.2 parts of dispersible rubber powder, 10 to 16 parts of fatty acid triglyceride, 0.6 to 1 part of a Ca-Zn composite heat stabilizer, 4 to 10 parts of a carbide, 5 to 9 parts of sodium nitrite and 8 to 12 parts of a coupling agent. The waterproofing slurry has the beneficial effects of being capable of well bonding with a base surface, difficult to fall, short in curing drying time, and excellent in mildew resistance, weatherability and waterproofness.
Waterproofing slurry
LIU GUOLEI (author)
2015-11-11
Patent
Electronic Resource
English
IPC:
C04B
Kalk
,
LIME